Eddy Current Test

How can the ferrous sulfate layer affect the Eddy Current Test?

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 889

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
889
19:58 Mar-04-2018
Re: Eddy Current Test
In Reply to Alejandro Dominguez at 21:31 Feb-28-2018 (Opening).

Alexandro,

You only speak of the surface layer, but don't mention the material used in the remainder of the tube.

One thing for sure, the ferrous sulfate layer will influence the Eddy Current because of the constant variation in permeability. I would therefore recommend the use of RFT for this inspection.

 
 Reply 
 
Kalaivanan
Kalaivanan
09:28 Mar-05-2018
Re: Eddy Current Test
In Reply to Michel Couture at 19:58 Mar-04-2018 .

Presence any Fe content in a tube may influence the magnetic properties.
It require a DC coil or permanent magnet to saturate the tube before Eddy testing.

****RFET, MFL and IRIS are recommended**

 
 Reply 
 
Alejandro Dominguez
Cuba, Joined May 2011, 2

Alejandro Dominguez

Cuba,
Joined May 2011
2
14:51 Mar-05-2018
Re: Eddy Current Test
In Reply to Michel Couture at 19:58 Mar-04-2018 .

The number of tubes is 15,000, the predominant material of the tubes is aluminum brass. There is another zone that has nickel cupro, but it is around 5% of the total of tubes

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window