Coarse grained material

During ultrasonic testing in coarse grained material velocity will increase or decrease why?

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 897

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
897
23:53 Jul-10-2018
Re: Coarse grained material
In Reply to Yoganathan at 06:35 Jul-10-2018 (Opening).

what happens with a coarse grain material is that it will attenuate the sound beam. You will therefore be required to decrease your frequency. Many procedure suggest 1 or even 0.5 MHz.

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 897

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
897
04:14 Jul-11-2018
Re: Coarse grained material
In Reply to Yoganathan at 06:35 Jul-10-2018 (Opening).

what happens with a coarse grain material is that it will attenuate the sound beam. You will therefore be required to decrease your frequency. Many procedure suggest 1 or even 0.5 MHz.

 
 Reply 
 
SULTAN KHAN
Engineering, NDT SUPERVISOR
MK FASTENERS BOMMASANDRA BANGALORE, India, Joined Jun 2017, 2

SULTAN KHAN

Engineering, NDT SUPERVISOR
MK FASTENERS BOMMASANDRA BANGALORE,
India,
Joined Jun 2017
2
10:37 Jul-11-2018
Re: Coarse grained material
In Reply to Yoganathan at 06:35 Jul-10-2018 (Opening).

BECAUSE OF ATTENUATION OF MOLECULES BETWEEN THEM SO THAT IS REASON TO DECREASE A VELOCITY

 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window