Establishing a Certification for EMAT Ultrasonic NDE

I am a consultant working with itRobotics in the Houston, Texas area (www.itrobotics.com). itRobotics is commercializing EMATs for applications within several industrial sectors. Some potential users of these NDE inspection services have inquired about having some of their inspection technicians trained to perform an independent assessment of inspection issues for their suitability to benefit them from one or more of the cost, environmental or other advantages that may be inherent in an EMAT-based inspection. The experience of itRobotics as well as my own personal experience is that a large majority of NDT technicians or engineers possessing Level III UT certification are not equipped to perform EMAT-based test evaluations. Currently, I do the training as well as EMAT test assessment suitability for itRobotics. This could certainly be viewed by a prospective client as not being an independent test assessment and evaluation. I have been asked by itRobotics to look into establishing an independent training and certification program through some appropriate professional organization. I am posting here to solicit feedback from the ultrasonic NDE/NDT community on which body or bodies might be most appropriate as the “certification authority”.

 
 Reply 
 
ASHOK KUMAR PATRA
,
Saudi K-KEM Engineering service co, Saudi Arabia, Joined May 2018, 55

ASHOK KUMAR PATRA

,
Saudi K-KEM Engineering service co,
Saudi Arabia,
Joined May 2018
55
12:25 Feb-17-2019
Re: Establishing a Certification for EMAT Ultrasonic NDE
In Reply to Bruce Maxfield at 00:36 Feb-17-2019 (Opening).

EMAT is a technique of Ultrasonic testing. Only you use magnetostriction for sound generation then data acquisition and plotting A-scan B-scan or C-scan. You have to calibrate machine as per UT only.

So level-III in UT can provide this training provided he has good knowledge of EMAT machine.


Or he will change your procedure and nominate you as a trainer in your procedure for qualification of level-I/ level-II technicians and himself.


Then he will arrange for test as per ASNT-TC -1A . General min 40 questions, Specific 20 questions min, Practical and Reporting.


signing authority as per ASNT a Level-III UT.


If only machine operator you yourself can provide training.

 
 Reply 
 
Petronext International
Petronext International
07:55 Feb-19-2019
Re: Establishing a Certification for EMAT Ultrasonic NDE
In Reply to Bruce Maxfield at 00:36 Feb-17-2019 (Opening).

So level-III in UT can provide this training provided he has good knowledge of EMAT machine.

 
 Reply 
 
ASHOK KUMAR PATRA
,
Saudi K-KEM Engineering service co, Saudi Arabia, Joined May 2018, 55

ASHOK KUMAR PATRA

,
Saudi K-KEM Engineering service co,
Saudi Arabia,
Joined May 2018
55
09:46 Feb-19-2019
Re: Establishing a Certification for EMAT Ultrasonic NDE
In Reply to Petronext International at 07:55 Feb-19-2019 .

Dear,

If he has good knowledge and have a certificate of training from the machine manufacturer is better.
so the proof of some training and good practical and reporting.

 
 Reply 
 
Volkan Eritmen
Sales,
Innerspec Technologies, Spain, Joined Jan 2019, 5

Volkan Eritmen

Sales,
Innerspec Technologies,
Spain,
Joined Jan 2019
5
12:03 Feb-19-2019
Re: Establishing a Certification for EMAT Ultrasonic NDE
In Reply to ASHOK KUMAR PATRA at 09:46 Feb-19-2019 .

We, Innerspec Technologies, are providing EMAT trainings for our customers. They could focus on a specific application such as High Temperature Thickness Measuremen, Residual Stress Measurement or Corrosion Detection Under Pipe Support or simply they could get a full EMAT training includes all of our main applications.

For more information please contact me: veritmen@innerspec.com

 
 Reply 
 
Clair D'El Rei
NDT Inspector,
I am looking for a new opportunity in the labor market and I accept proposals from other countries i, Brazil, Joined Feb 2019, 15

Clair D'El Rei

NDT Inspector,
I am looking for a new opportunity in the labor market and I accept proposals from other countries i,
Brazil,
Joined Feb 2019
15
19:25 Feb-20-2019
Re: Establishing a Certification for EMAT Ultrasonic NDE
In Reply to Bruce Maxfield at 00:36 Feb-17-2019 (Opening).

Good afternoon;
I am an Inspector in UT-ASNT TC1A/ISO9712 e UT SNQC/ABENDI-BRASIL / ISO9712.
I would like to receive more information about this application method for inspection.

 
 Reply 
 

Product Spotlight

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>