ut of carbon steel shaft
Please can somebody suggest me to do UT of carbon steel shaft size of 320 dia and 4200 length. I have been told by UT inspector level 2 straight beam transducer never be used for crack detection it is only used for lamination or thickness. Is it so.
Shaft can be inspected radially and axially with straight beam or angle beam transducer.
 
 Reply 
 
Daniel Braun
Daniel Braun
10:11 May-10-2019
Re: ut of carbon steel shaft
In Reply to Sheeraz at 21:07 May-09-2019 .

In-service inspection - detection of transverse cracks:

http://www.sonotronndt.com/SHAFTS_BOLTS.htm

http://www.sonotronndt.com/APPLICATIONS/PA_APPS/PA_APP_STORE/ISONIC_PA_EXPERT_SHAFT.pdf

http://www.sonotronndt.com/RW_AXLE.htm

http://www.sonotronndt.com/APPLICATIONS/PA_APPS/PA_APP_STORE/ISONIC_PA_RW_AXLE_TEST.pdf

In-service inspection - detection of longitudinal cracks:

http://www.sonotronndt.com/RODSCAN.htm

http://www.sonotronndt.com/APPLICATIONS/PA_APPS/PA_APP_STORE/ISONIC_PA_ROD_Scan.pdf

Both inspection are applicable for the hollow and solid shafts








1
 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 893

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
893
12:46 May-13-2019
Re: ut of carbon steel shaft
In Reply to Sheeraz at 21:07 May-09-2019 .

ASTM E388

 
 Reply 
 
Sheeraz
NDT Inspector,
Pakistan, Joined Jan 2014, 3

Sheeraz

NDT Inspector,
Pakistan,
Joined Jan 2014
3
20:10 May-15-2019
Re: ut of carbon steel shaft
In Reply to Michel Couture at 12:46 May-13-2019 .

Thank you all please share acceptance criteria for in service shaft

 
 Reply 
 
Daniel Braun
Daniel Braun
09:45 May-16-2019
Re: ut of carbon steel shaft
In Reply to Sheeraz at 20:10 May-15-2019 .

for the in-service inspection for fatigue transverse cracks the sensitivity setting is based on the detection of standard saw cut made from the rounded surface of the shaft at rectangle to the axis, the depth of the saw cut for each area of the shaft is defined by the local procedures and regulations, for example for the same type of railway car shaft - wheel-seat area - the depth may vary from 0.5 to 3 mm in different countries

 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window