ASTM 2175 Requirements of penetrant inspection

Hi,
Did someone work with this standard in refer to PT.
I need information about what is subject of evaluation discontinuities or indications??
Thank in advance.

 
 Reply 
 
SUMURAY
SUMURAY
18:45 Aug-21-2019
Re: ASTM 2175 Requirements of penetrant inspection
In Reply to Grzegorz at 11:52 Aug-21-2019 (Opening).

Excuse me SIR.
are you sure of this standard is correct?
I Think is ASTM E1417 or ASTM E165.

 
 Reply 
 
Grzegorz
NDT Inspector,
Poland, Joined Feb 2012, 15

Grzegorz

NDT Inspector,
Poland,
Joined Feb 2012
15
08:00 Aug-22-2019
Re: ASTM 2175 Requirements of penetrant inspection
In Reply to SUMURAY at 18:45 Aug-21-2019 .

Sie,
You're right, these mentioned by you standards refer to PT, but both contain only parameters for carring out of test.
ASTM 2175 contains only requirements of all NDT tests among others PT.

 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window