Finding Debonding between composites

Hello All,

Could anyone help me out with below mentioned two different cases

Case I- Sandwich structure made of Carbon Steel (CS-5 mm) + Polyurethane (PU-10 mm) + Carbon Fibre (CF-10mm). is there any practical solution to find debonding(planner or volumetric) between Interface 1(CS-PU) and Interface 2 (PU-CF).
Access for UT from only one side (Carbon steel side)

Case II- Sandwich structure made of CF (15 mm)+ PU(15mm) + CF (10 mm).
Same finding as Case I.
Access from only one side.

 
 Reply 
 
Wiesław Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 273

Wiesław Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
273
10:37 Aug-23-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

Immersion or contact testing should be possible in the first case, but it will be necessary to use transducer with quite short pulse and quite sophisticated signal analysis, since the difference between total reflection and transmission into plastic is not very strong and many internal reflexions in steel can be expected.
Second case is more difficult due to the fact, that CF and PU are not very different and CF is quite attenuating. It should work, but requires careful development of suitable procedures.

2
 
 Reply 
 
Anand
India, Joined Jul 2016, 1

Anand

India,
Joined Jul 2016
1
10:40 Aug-23-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

Hi,
Myself Anand.

I think UT will work for composites.Based on my work experience I'm telling. But the combination of metal and composites, I am not sure.

Thanks.

1
 
 Reply 
 
Daniel Braun
Daniel Braun
12:49 Aug-23-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

Generally it is possible, if you have the samples available - you may ship them to Sonotron NDT A-Lab for performing the trials and laying out the necessary setup (instrument, probe, settings) - if you're interesting simply e-mail and we'll proceed further. The service is FOC

 
 Reply 
 
Andres Romero
NDT Inspector,
Spain, Joined Jul 2019, 9

Andres Romero

NDT Inspector,
Spain,
Joined Jul 2019
9
04:26 Aug-24-2019
Re: Finding Debonding between composites
In Reply to Jignesh Dhimar at 07:59 Aug-23-2019 (Opening).

zoom image



Hello, sorry for my English is not good.
If possible, by immersion. With squirt machine.
Several frequencies are needed.
 
 Reply 
 

Product Spotlight

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window