PAUT Probe and Wedge compatibility

Dear experts,
Can we use Olympus PAUT Probes and Wedges in Sonatest Equipment. If so how we can use? We need to create focal law in other software and import to sonatest? Can anyone help me on this

Thanking you in advance

 
 Reply 
 
Levi Porter
R & D,
Dacon Inspection Technologies, Thailand, Joined Jan 2017, 60

Levi Porter

R & D,
Dacon Inspection Technologies,
Thailand,
Joined Jan 2017
60
11:20 Mar-22-2020
Re: PAUT Probe and Wedge compatibility
In Reply to ARJUN VIJAY at 10:59 Mar-22-2020 (Opening).

HI Arjun,
It's been some time since I've used a VEO+, however I am sure they have the option to add custom probes and wedges into their library. Once you've added the parameters the unit should be able to create the focal laws without issue. You may also be able to use ESBeamtool to import focal laws but I do not know about the compatibility for Sonatest.

 
 Reply 
 
JohnP
R & D,
Sonomatic Ltd, United Kingdom, Joined Sep 2016, 9

JohnP

R & D,
Sonomatic Ltd,
United Kingdom,
Joined Sep 2016
9
16:13 Mar-22-2020
Re: PAUT Probe and Wedge compatibility
In Reply to Levi Porter at 11:20 Mar-22-2020 .

Dear Arjun,
Levi is correct that Olympus probes and wedges can be used with the Veo+.
If the wedges and probes do not appear in the Veo libraries then the values can be entered manually.
Just beware that the terminology of the probe parameters and wedge parameters can be different for omniscan and Sonatest.
Regards
John

1
 
 Reply 
 
Paul Holloway
Consultant,
Holloway NDT & Engineering Inc , Canada, Joined Apr 2010, 242

Paul Holloway

Consultant,
Holloway NDT & Engineering Inc ,
Canada,
Joined Apr 2010
242
19:26 Mar-22-2020
Re: PAUT Probe and Wedge compatibility
In Reply to ARJUN VIJAY at 10:59 Mar-22-2020 (Opening).

If you contact your local Sonatest rep, they should be able to provide you with a probe database of many different probe types.

Or as Levi and John say, you can make them yourself. It's quite simple and takes only a few minutes each. Then just save them on your Veo and you'll never have to do it again.

P

1
 
 Reply 
 
Arman
Engineering,
Turkey, Joined Oct 2014, 42

Arman

Engineering,
Turkey,
Joined Oct 2014
42
15:41 Mar-24-2020
Re: PAUT Probe and Wedge compatibility
In Reply to Paul Holloway at 19:26 Mar-22-2020 .

Hi Arjun,

Both Paul and John are correct, I had same concern, I contacted Sonatest about this, they provided me with wedge/probe database that you can put into your PA machine and load into your setting. I do strongly recommend to check beam exit points as sometimes databases are not 100% correct. In my case, I observed around 10 mm exit point off! I did edit wedge parameters to get the correct exit point as I simulated with ESBeamtools software.
Hope this helps
Arman

 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>