03:28 Oct-23-2005
NDT- procedures for tubular axles.


Dear friends !

I am looking for a NDT procedures at tubular axles
(railway underground systems).If somebody can help me,
please send me an answer as soon as possible.

Thank You !


 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
02:40 Oct-24-2005
Re: NDT- procedures for tubular axles.
Dear Sir,

There are several AAR and European standards available for axle testing of rail cars for both passenger and industrial purposes. Which one would govern your case would be determined by your local transportation authority and/or the owner of the rail cars.

I have also had contact with Lavender NDT in this regard, they provide an excellent level of consulting services for the rail industry.

An alternative would also be the BHP Rail Institute in Melbourne Australia.

Regards,

David Hermanutz
RTD Quality Services
Pipeline Integrity
North America


----------- Start Original Message -----------
:
: Dear friends !
: I am looking for a NDT procedures at tubular axles
: (railway underground systems).If somebody can help me,
: please send me an answer as soon as possible.
: Thank You !
------------ End Original Message ------------




 
 Reply 
 
A-A-AMIRI
Consultant, NDT/QC/WELD INSPECTION
Iran, Joined Nov 2005, 20

A-A-AMIRI

Consultant, NDT/QC/WELD INSPECTION
Iran,
Joined Nov 2005
20
07:58 Nov-01-2005
Re: NDT- procedures for tubular axles.
----------- Start Original Message -----------
: Dear Sir,
YOU CAN USE OF UIC STANDARD RAIL ROAD INDUSTRY.


 
 Reply 
 

Product Spotlight

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>