00:26 Jul-13-1999
Measurement of Hydrogen attack in steel pipe

Can anyone help me to suggest the most accurate ultrasonic procedure to measure
the presence of hydrogen attack in steel pipes applicable to petrochemical industry. I
assume that attenuation measurement, backwall echo measurement or
velocity measurements(thus the poisson ratio) can be used but I am now sure of thier
accuracy? Is there any acceptance and rejection criteria for
evaluating the severity level of this hydrogen attack?

Your urgent reply is highly appreciated.
Thank you.


 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
02:56 Jul-13-1999
Re: Measurement of Hydrogen attack in steel pipe
: Can anyone help me to suggest the most accurate ultrasonic procedure to measure
: the presence of hydrogen attack in steel pipes applicable to petrochemical industry. I
: assume that attenuation measurement, backwall echo measurement or
: velocity measurements(thus the poisson ratio) can be used but I am now sure of thier
: accuracy? Is there any acceptance and rejection criteria for
: evaluating the severity level of this hydrogen attack?

: Your urgent reply is highly appreciated.
: Thank you.


AEA technology have done a lot of good work in this area utilizing TOFD,
try Jan.Verkooijen@aea-technology.nl



 
 Reply 
 
Brian Shannon
Brian Shannon
02:32 Aug-11-1999
Re: Measurement of Hydrogen attack in steel pipe
: : Can anyone help me to suggest the most accurate ultrasonic procedure to measure
: : the presence of hydrogen attack in steel pipes applicable to petrochemical industry. I
: : assume that attenuation measurement, backwall echo measurement or
: : velocity measurements(thus the poisson ratio) can be used but I am now sure of thier
: : accuracy? Is there any acceptance and rejection criteria for
: : evaluating the severity level of this hydrogen attack?

: : Your urgent reply is highly appreciated.
: : Thank you.

:
: AEA technology have done a lot of good work in this area utilizing TOFD,
: try Jan.Verkooijen@aea-technology.nl

Suggest you contact iesconde.com for further information regarding this mechanism.


 
 Reply 
 

Product Spotlight

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window