Joerg Neubert
Joerg Neubert
08:32 Feb-24-1999
UT of filled or unfilled pipes

I got the task to find out if there`s a difference in
mechanized UT of pipes under unfilled and filled
conditions (by water) as a 1st measurement (basis) for
the in-service inspection of Nuclear power plants.
Who knows some literature and where were made such
examinations?
I hope You, the ndt.net users can help me.
Thanks in advance.
Joerg (e-mail please see above)
phone: +49 9131 18 7895 fax: +49 9131 18 2053



 
 Reply 
 
Rainer Meier
R & D
retired from intelligeNDT Systems & Services, Germany, Joined Nov 1998, 15

Rainer Meier

R & D
retired from intelligeNDT Systems & Services,
Germany,
Joined Nov 1998
15
04:47 Feb-25-1999
Re: UT of filled or unfilled pipes
: I got the task to find out if there`s a difference in
: mechanized UT of pipes under unfilled and filled
: conditions (by water) as a 1st measurement (basis) for
: the in-service inspection of Nuclear power plants.
: Who knows some literature and where were made such
: examinations?
: I hope You, the ndt.net users can help me.
: Thanks in advance.
: Joerg (e-mail please see above)
: phone: +49 9131 18 7895 fax: +49 9131 18 2053




 
 Reply 
 
Rainer Meier
R & D
retired from intelligeNDT Systems & Services, Germany, Joined Nov 1998, 15

Rainer Meier

R & D
retired from intelligeNDT Systems & Services,
Germany,
Joined Nov 1998
15
05:27 Feb-25-1999
Re: UT of filled or unfilled pipes
Dear Mr. Neubert,

the echo of a backwall or a reflector is influenced by the
media behind the backwall/reflector. In practice this effect
can normally be neglected.
In the case of a longitudinal wave in a steel pipe wall, the
reflection coefficient changes from nearly 1 (air filling) to
0.937 for the water filled pipe. That means, that the loss of
backwall amplitude due to the water filling is less than 0.6 dB.
This can be neglected compared with other effects to the signal
amplitude, e.g. changing coupling conditions.

In the case of shear waves, the amplitude loss due to water
filling might be slightly higher, but does not exceed 1 dB.
(The shear wave impedance is smaller then the long wave
impedance).

Additional, water film or water drops can cause unwanted
echos. If there is a waterfilm on the backwall of a component,
the echo from the waterfilm surface may interfere with the
components backwall echo. But due to the fact, that only
12 percent of the sound energy penetrates the backwall,
this effect is also not significant.

The normally used UT-waves are only minor influenced by
the water filling. This also includes creeping waves and
long-shear wave conversion. Rayleigh waves are much more
influenced, through a high damping caused by the water and
through reflections caused by water drops.

The above mentioned facts are valid for steel pipes. If you
think about other materials, e.g. aluminum pipes with a
much lower acoustic impedance, the water filling will have
a higher influence!

Rainer Meier

: I got the task to find out if there`s a difference in
: mechanized UT of pipes under unfilled and filled
: conditions (by water) as a 1st measurement (basis) for
: the in-service inspection of Nuclear power plants.
: Who knows some literature and where were made such
: examinations?
: I hope You, the ndt.net users can help me.
: Thanks in advance.
: Joerg (e-mail please see above)
: phone: +49 9131 18 7895 fax: +49 9131 18 2053




 
 Reply 
 
Mark
NDT Inspector
USA, Joined Oct 2009, 52

Mark

NDT Inspector
USA,
Joined Oct 2009
52
00:06 Feb-05-2012
Re: UT of filled or unfilled pipes
In Reply to Rainer Meier at 05:27 Feb-25-1999 .

So shear wave weld inspection of a filled water vessel shouldn't be an issue? You say that 12 percent of the amplitude is lost off the back wall reflection but the say only 1 db is lost for shear wave. I don't understand how that is....if 12 percent is lost and your running at 50 db it would be 12 percent of 50db right? That's alot mor then 1 db.

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
15:04 Feb-05-2012
Re: UT of filled or unfilled pipes
In Reply to Joerg Neubert at 08:32 Feb-24-1999 (Opening).

zoom image



Joerg, we had a similar task 30 years ago, to assess the effect of water in the vessel when doing periodic inspection. The easiest option was to evaluate the effect on our DAC curve. Of course in the first half skip there is no effect, only after reflection off the steel water interface does the problem show itself. To determine how significant this is there is an easy setup. We placed our calibration block in a tray (about 50mm deep) large enough to hold the calibration block. Under each end of the block we placed a square bar that allowed us to raise the block off the tray surface about 10mm. Then draw your DAC. You can draw it first with no water then again after adding a small amount to contact the skip surface and see the difference in effect. There will be a difference based on the angle used!
 
 Reply 
 
Mark
NDT Inspector
USA, Joined Oct 2009, 52

Mark

NDT Inspector
USA,
Joined Oct 2009
52
16:19 Feb-05-2012
Re: UT of filled or unfilled pipes
In Reply to Ed Ginzel at 15:04 Feb-05-2012 .

Ed,

What was the loss of sound due to transmission in the water? Would you consider the effect unsignificant? Does it exceed 1 dB for shear wave inspections? When i calculate the reflection coeffecient of a shear wave through steel into water nearly 20 percent of the sound is transmitted into the water, I would think this would be significant due to the fact that when the sound beam strikes a defect it will propagate back to the transducer in the same path it came, meaning a defect in the second leg would have a sound beam that contacts the water surface twice ( Lossing 40 percent of its sound, or nearly 6 db). Is this safe to assume Ed?

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
16:50 Feb-05-2012
Re: UT of filled or unfilled pipes
In Reply to Mark at 16:19 Feb-05-2012 .

Mark, the effect is not insignificant. The DAC points after the skip typically dropped 2dB. But this is not a constant and will be different for different angles.

 
 Reply 
 
Mark
NDT Inspector
USA, Joined Oct 2009, 52

Mark

NDT Inspector
USA,
Joined Oct 2009
52
23:51 Feb-05-2012
Re: UT of filled or unfilled pipes
In Reply to Ed Ginzel at 16:50 Feb-05-2012 .

Ed,

You say roughly a 2 db loss, with a 40 percent transmission loss in the water wouldn't it be closer to a 5 db loss? Can you explain? Also, I'd your calibrating for a weld that is 3/8" thick on a 3/4" block how can you compensate for the water loss in the second half skip due to the fact you will not get to the water on the calibration block until 3/4" deep but will be in the second leg of the weld after 3/8"???

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
03:22 Feb-06-2012
Re: UT of filled or unfilled pipes
In Reply to Mark at 23:51 Feb-05-2012 .

Mark, have you tried the simple setup I suggested? It took me all of 5 minutes to verify on a single point. You will note from Krautkramer's echo-transmittance curves that the equation in the third English edition (A.17) is for the incidence from the liquid. But the result can be derived for incidence from the solid. In the simple perpendicular incidence case the Java applet on http://www.ndt-ed.org/EducationResources/CommunityCollege/Ultrasonics/Physics/applet_2_7/applet_2_7.htm predicts a 2dB for the one-way path for the 0 degree condition reflection! In pulse-echo the beam returns along the same path so another 2dB would be lost. The setup I used was for a 60° on the IOW block so the loss is not the same as for 0 degree. I peaked the signal at 100% and held the probe in place as I placed it on the water...the signal dropped to about 81% (near enough to 2dB). The math is nice, but it is always useful to validate by actually doing the hands-on.

 
 Reply 
 
Andrey Bazulin
R & D, -
Scientific Center ECHO+, Russia, Joined Sep 2006, 58

Andrey Bazulin

R & D, -
Scientific Center ECHO+,
Russia,
Joined Sep 2006
58
18:13 Feb-06-2012
Re: UT of filled or unfilled pipes
In Reply to Ed Ginzel at 03:22 Feb-06-2012 .

Ed!

What do you think - is this a good job for CIVA to give an answer?

I think that aspect of sound propagation from boundaries is taken into account in "pencil" method.

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
13:31 Feb-08-2012
Re: UT of filled or unfilled pipes
In Reply to Andrey Bazulin at 18:13 Feb-06-2012 .

zoom image

Skip Air versus Water

Andrey, good idea! I uploaded the model image summary. I ran 2 probe angle models, 45° and 60° with a direct path to a 3mm SDH and a skip path using a 50mm steel block model. When plotting the echo dynamics as the probe is moved past the SDH, the peaks indicate the points we would use to draw a DAC. When water is used at the skip point we see the amplitude drop 1.6dB for the 45° beam and 1.4 for the 60° beam. In my earlier post I made a physical measurement with the 60° beam and said the signal dropped from 100% to 81%. That is 1.8dB from the physical measurement. Civa predicts 1.6dB. Further to Joerg's concerns for literature search, there may be a report on a similar effect in CANDU feeder tube inspections. There they made provision for amplitude corrections at each skip point on the steel-water interface. But I think the Civa results could be used in technical justifications.
 
 Reply 
 
Andrey Bazulin
R & D, -
Scientific Center ECHO+, Russia, Joined Sep 2006, 58

Andrey Bazulin

R & D, -
Scientific Center ECHO+,
Russia,
Joined Sep 2006
58
19:28 Feb-08-2012
Re: UT of filled or unfilled pipes
In Reply to Ed Ginzel at 13:31 Feb-08-2012 .

Thank you Ed!

I think that I will try try to repeat this experiment in our CIVA verification task. 0.2 dB - it is very good result.

 
 Reply 
 

Product Spotlight

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window