mudiharyanto
mudiharyanto
00:20 Aug-09-1999
TCG

Dear Sir,
I am very interesting to see your nice homepage.
Please help me Sir, I want to know information about the Time Corrected Gain Ultrasonic (TCG-theoritical)).

Thanks a lot for this matter.

Best Regards,
Mudi Haryanto
NDT Inspector


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 616

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
616
02:29 Aug-09-1999
Re: TCG
Defination of "TCG"

Time-dependent gain (TDG)

Time dependent or swept gain function fitted to some ultrasonic instruments to
correct for the distance related reduction in reflected amplitude.
Editor comment: Usually called DAC 'distance amplitude correction' or TCG 'time controlled gain'

This definitions is used in the standard EN 12688-1 "Characterization and verification of ultrasonic examination -
Part 1: Instruments" For other definations the EN 1330 shall apply.
http://www.ndt.net/article/ut_az/ut_u/info/def_eq.htm

----------------
: Dear Sir,
: I am very interesting to see your nice homepage.
: Please help me Sir, I want to know information about the Time Corrected Gain Ultrasonic (TCG-theoritical)).

: Thanks a lot for this matter.

: Best Regards,
: Mudi Haryanto
: NDT Inspector




 
 Reply 
 
mudi haryanto
mudi haryanto
03:56 Aug-10-1999
Re: TCG
: Dear Sir,
Thanks for response soon,
I have an USD 10 (krautkramer), and for reject of assumption I used TCG. My question is how to applied and procedure of TCG ?
I can operate TCG corresponding to manual USD 10 but I don't know to apply for reject.
is the TCG include ASME, DGS, or AWS standard ?
I want to change information, may be everbody do you have experience to use USD 10 ?


Thanks

Mudi haryanto


 
 Reply 
 
E. Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1300

E. Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1300
03:48 Aug-10-1999
Re: TCG
Mudi:
ASME Section V Article 4 Appendix B Gives instructions on how to construct a Distance Amplitude Correction curve to set your primary sensitivity.
These instructions are for the "traditional" curve drawing marked directly on the screen. However, the CURVE is one option for the amplitude correction that is required with increasing soundpath.
When you go to the main body of ASME Section V Article 5 T-542.4.3 (as well as Article 4 Appendix B) it states that other techniques for calibrating angle beams may be used.
Since TCG (Time Corrected Gain) is merely a convenient method of increasing gain as distance along the timebase increases, this effectively allows you to provide the same sort of compensation to sensitivity as is provided with the DAC curve.
The advantage of the TCG is that for greater distances the signals to evaluate are a smaller percentage of the total screen height when using a DAC curve.
But when TCG is used the signals evaluated for 20% of the Reference sensitivity are the same screen height at 90% of the screen range (soundpath) as they are at 20% of the screen range.

I do not know the requirements for AWS but the wording in ASME obviously permits TCG.

Ed

: : Dear Sir,
: Thanks for response soon,
: I have an USD 10 (krautkramer), and for reject of assumption I used TCG. My question is how to applied and procedure of TCG ?
: I can operate TCG corresponding to manual USD 10 but I don't know to apply for reject.
: is the TCG include ASME, DGS, or AWS standard ?
: I want to change information, may be everbody do you have experience to use USD 10 ?

:
: Thanks

: Mudi haryanto




 
 Reply 
 
joseph
joseph
00:44 Mar-01-2000
Re: TCG
: Dear Sir,
: I am very interesting to see your nice homepage.
: Please help me Sir, I want to know information about the Time Corrected Gain Ultrasonic (TCG-theoritical)).

: Thanks a lot for this matter.

: Best Regards,
: Mudi Haryanto
: NDT Inspector




 
 Reply 
 

Product Spotlight

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window