UT inspections of large castings and austenitic steel

What techniques are available to inspect (volumetric) coarse grain
material,such as castings and austenitic steels, with a thick cross
section? Examples where this material would be used is in the
primary loop of nuclear power stations, and in pipe work in the
petrochemical industry.

Thanks


 
 Reply 
 
jayesh.vanza
jayesh.vanza
07:53 Aug-11-1999
Re: UT inspections of large castings and austenitic steel
: What techniques are available to inspect (volumetric) coarse grain
: material,such as castings and austenitic steels, with a thick cross
: section? Examples where this material would be used is in the
: primary loop of nuclear power stations, and in pipe work in the
: petrochemical industry.

: Thanks




 
 Reply 
 
GAF
GAF
03:16 Aug-13-1999
Re: UT inspections of large castings and austenitic steel
: : What techniques are available to inspect (volumetric) coarse grain
: : material,such as castings and austenitic steels, with a thick cross
: : section? Examples where this material would be used is in the
: : primary loop of nuclear power stations, and in pipe work in the
: : petrochemical industry.

: : Thanks

Depends on the material and what type of inspection but in general Ultrasonic inspection of CSS components has been unreliable. Your best bet is a low freqency focused dual L wave 3/4 or 1 meg for crack detection



 
 Reply 
 
Norm Woodward
Norm Woodward
08:42 Aug-13-1999
Re: UT inspections of large castings and austenitic steel
: What techniques are available to inspect (volumetric) coarse grain
: material,such as castings and austenitic steels, with a thick cross
: section? Examples where this material would be used is in the
: primary loop of nuclear power stations, and in pipe work in the
: petrochemical industry.

I have no first hand experience with them, but Krautkramer, and a few others, were pushing "composite transducers" as a solution to inspecting noisy materials.

As I recall, this site had some on-line articles about them back in the fall of '96.

Hope this helps,

Norm


 
 Reply 
 
Russ Minkwitz
Russ Minkwitz
09:59 Aug-13-1999
Re: UT inspections of large castings and austenitic steel
: What techniques are available to inspect (volumetric) coarse grain
: material,such as castings and austenitic steels, with a thick cross
: section? Examples where this material would be used is in the
: primary loop of nuclear power stations, and in pipe work in the
: petrochemical industry.

Sir,

Dual element critically refracted longitudinal waves have been used for such applications for years. They are mentioned in IIW handbook on the examination of austenetic welds.

Further there are more detailed papers on dual element and tandem techniques published by RTD and Panametrics.

If you would like copies please provide you address and we will send more information.

Best Regards,
Russ Minkwitz
Manager, Transducer Sales





 
 Reply 
 
satish
satish
09:38 Oct-29-1999
Re: UT inspections of large castings and austenitic steel
: What techniques are available to inspect (volumetric) coarse grain
: material,such as castings and austenitic steels, with a thick cross
: section? Examples where this material would be used is in the
: primary loop of nuclear power stations, and in pipe work in the
: petrochemical industry.

: Thanks




 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window