5213 views
Technical Discussions
MATTHEW GODFREY Genaeral Motors-(Vauxhall UK)
MATTHEW GODFREY Genaeral Motors-(Vauxhall UK)
01:23 Aug-19-1999
Ultrasonic Testing of spot welds

I need some Information with regards to Ultrasonic testing of spot
welds, if anyone has any information please contact me on the above
E-mail location, I am open to discusion and would appreciate any
correspondance.


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
00:07 Aug-19-1999
Re: Ultrasonic Testing of spot welds
: I need some Information with regards to Ultrasonic testing of spot
: welds, if anyone has any information please contact me on the above
: E-mail location, I am open to discusion and would appreciate any
: correspondance.
---------------

Inspection of Spot Welds was several times discussed in this Forum,
however it is still interesting to discuss what's new.
You may use the Forum Search to find the previous discussions.
Articles can be found with the article power search also.
Anyway, something new was published recently at the annual DGZfP conference May 1999 in Celle.
See below the German abstracts:

http://www.ndt.net/abstract/dgzfp99/data/7.htm
K.-H. Fischer, S. Schreiber, Duisburg; H. Wüstenberg, Berlin
Möglichkeiten der zerstörungsfreien Prüfung von Widerstandspunktschweißverbindungen.
Author Contact:
H. Wüstenberg at http://www.ndt.net/wshop/forum/particip/221.htm

http://www.ndt.net/abstract/dgzfp99/data/p4.htm
C. Köhler, Burgwedel; F. Alich, Bremen; H.-L. Vellen, Schleiden
Ultraschallprüfung von widerstandsgeschweißten Punkten in der Produktion
der Automobilindustrie - Umsetzung und effektive Nutzung
Author Contact:
C. Köhler via G. Vogt at http://www.ndt.net/wshop/forum/particip/213.htm



 
 Reply 
 
Ing. Manuel Haces Valdez
Ing. Manuel Haces Valdez
00:16 Aug-20-1999
Re: Ultrasonic Testing of spot welds
: I need some Information with regards to Ultrasonic testing of spot
: welds, if anyone has any information please contact me on the above
: E-mail location, I am open to discusion and would appreciate any
: correspondance.

Very good information Rolf pointed out. I have some experience with
UT inspection in spot welds. If you need further information let me know.
Regards.



 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
07:38 Aug-21-1999
Re: Ultrasonic Testing of spot welds



 
 Reply 
 
Wieslaw Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 276

Wieslaw Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
276
00:17 Aug-25-1999
Re: Ultrasonic Testing of spot welds

: I need some Information with regards to Ultrasonic testing of spot
: welds, if anyone has any information please contact me on the above
: E-mail location, I am open to discusion and would appreciate any
: correspondance.

We have scanned spot welds with a short pulse transducer (100 ns pulse length) and it works very good.
We can make a hand-held scanner for this purpose (we have designed and made similiar scanner for investigation of soft palate,
see please: http://www.optel.com.pl/article/english/plate.htm).

Wieslaw Bicz
(http://www.optel.com.pl)



 
 Reply 
 
Wuestenberg, Hermann
R & D
BAM Berlin, Germany, Joined Nov 1998, 26

Wuestenberg, Hermann

R & D
BAM Berlin,
Germany,
Joined Nov 1998
26
03:56 Sep-02-1999
Re: Ultrasonic Testing of spot welds
: I need some Information with regards to Ultrasonic testing of spot
: welds, if anyone has any information please contact me on the above
: E-mail location, I am open to discusion and would appreciate any
: correspondance.

The german society for NDT just published the reports of its Annual conference in Celle May 1999.
You may find there a survey on possibilities, entitled:
"Moeglichkeiten der zerstörungsfreien Pruefung von Widerstandspunktschweissverbindungen"
K.-H. Fischer, S. Schreiber, SLV Duisburg; H.Wuestenberg, BAM Berlin





 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
04:29 Sep-02-1999
Re: Ultrasonic Testing of spot welds
Thanks for Mr. Wuesentberg's hint.
The abstract of this paper he refereed to is available at:
http://www.ndt.net/abstract/dgzfp99/data/7.htm (in German)

We hope to publish this and other full-texts soon.
Maybe also translated to English!

Rolf Diederichs

: : I need some Information with regards to Ultrasonic testing of spot
: : welds, if anyone has any information please contact me on the above
: : E-mail location, I am open to discusion and would appreciate any
: : correspondance.

: The german society for NDT just published the reports of its Annual conference in Celle May 1999.
: You may find there a survey on possibilities, entitled:
: "Moeglichkeiten der zerstörungsfreien Pruefung von Widerstandspunktschweissverbindungen"
: K.-H. Fischer, S. Schreiber, SLV Duisburg; H.Wuestenberg, BAM Berlin





 
 Reply 
 
JAYESH.VANZA
JAYESH.VANZA
02:02 Sep-18-1999
Re: Ultrasonic Testing of spot welds
i need some infomation on ut testing of welds


 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
02:58 Nov-17-2000
Re: Ultrasonic Testing of spot welds
: : I need some Information with regards to Ultrasonic testing of spot
: : welds, if anyone has any information please contact me on the above
: : E-mail location, I am open to discusion and would appreciate any
: : correspondance.
: ---------------

: Inspection of Spot Welds was several times discussed in this Forum,
: however it is still interesting to discuss what's new.
: You may use the Forum Search to find the previous discussions.
: Articles can be found with the article power search also.
: Anyway, something new was published recently at the annual DGZfP conference May 1999 in Celle.
: See below the German abstracts:

: http://www.ndt.net/abstract/dgzfp99/data/7.htm
: K.-H. Fischer, S. Schreiber, Duisburg; H. Wüstenberg, Berlin
: Möglichkeiten der zerstörungsfreien Prüfung von Widerstandspunktschweißverbindungen.
: Author Contact:
: H. Wüstenberg at http://www.ndt.net/wshop/forum/particip/221.htm

: http://www.ndt.net/abstract/dgzfp99/data/p4.htm
: C. Köhler, Burgwedel; F. Alich, Bremen; H.-L. Vellen, Schleiden
: Ultraschallprüfung von widerstandsgeschweißten Punkten in der Produktion
: der Automobilindustrie - Umsetzung und effektive Nutzung
: Author Contact:
: C. Köhler via G. Vogt at http://www.ndt.net/wshop/forum/particip/213.htm


Panametrics has experienced great success in Australia using the Epoch3 for spot weld testing. Our client is currently experiencing correlation to destructive testing in excess of 90%.

David Hermanutz
Panametrics Melbourne



 
 Reply 
 
andy cunningham
Consultant, NDT/QA QC/R&D
ASNT,PCN, Canada, Joined Feb 2000, 14

andy cunningham

Consultant, NDT/QA QC/R&D
ASNT,PCN,
Canada,
Joined Feb 2000
14
01:23 Apr-17-2001
Re: Ultrasonic Testing of spot welds
: : : : : I need some Information with regards to Ultrasonic testing of spot
: : : : : welds, if anyone has any information please contact me on the above
.
you may try the panimetric sonopen. it is small enough to go directly onto the spot and it has a short focal point.



 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
03:13 Apr-17-2001
Re: Ultrasonic Testing of spot welds
: : : : : : I need some Information with regards to Ultrasonic testing of spot
: : : : : : welds, if anyone has any information please contact me on the above
: .
: you may try the panimetric sonopen. it is small enough to go directly onto the spot and it has a short focal point.

Dear Sirs,

Panametrics offers the Epoch Series Digital Ultrasonic Flaw Detectors with an innovative software package and a large assortment of standard and customized transducers specifically designed for Ultrasonic Spotweld Inspection.

Our company and applications engineers have years of experience in the European, American and Asian automotive markets with a proven history of successful Ultrasonic Spotweld Testing equipment and technology.

Our Epoch Flaw detectors have an easy user interface and easy to understand presentation with most users trained to a correlation rate with destructive test means of 95% after our specialized training course.

If you would like more information on our products and training please contact Ethan Sandahl or myself at your convenience.

Best Regards,

David Hermanutz
NDT Applications Engineer
Panametrics Melbourne

PS I would advise against the use of the Sonopen as it has not been specifically designed for Spotweld Testing and may lead to false interpretations



 
 Reply 
 
L.M.BORKAR
Consultant
International Radiography Services, India, Joined Mar 2001, 1

L.M.BORKAR

Consultant
International Radiography Services,
India,
Joined Mar 2001
1
02:39 Apr-18-2001
Re: Ultrasonic Testing of spot welds
: : : : I need some Information with regards to Ultrasonic testing of spot
: : : : welds, if anyone has any information please contact me on the above
: : : : E-mail location, I am open to discusion .
.

In recent demonstration of Krautkramer, w. germany, i have observed new spot weld check UT machine with PC control. Kindly contact to Krautcramer



 
 Reply 
 
Bill Neyer
Bill Neyer
05:13 Apr-18-2001
Web Site Explaining Ultrasonic Testing of spot welds
Please visit the web site below for an explanation of this procedure -
http://www.panametrics.com/div_ndt/pages/applications/general/spotweld.shtml
.
: Panametrics offers the Epoch Series Digital Ultrasonic Flaw Detectors with an innovative software package and a large assortment of standard and customized transducers specifically designed for Ultrasonic Spotweld Inspection.
.
: Our company and applications engineers have years of experience in the European, American and Asian automotive markets with a proven history of successful Ultrasonic Spotweld Testing equipment and technology.
.
: Our Epoch Flaw detectors have an easy user interface and easy to understand presentation with most users trained to a correlation rate with destructive test means of 95% after our specialized training course.
.
: If you would like more information on our products and training please contact Ethan Sandahl or myself at your convenience.
.
: Best Regards,
.
: David Hermanutz
: NDT Applications Engineer
: Panametrics Melbourne
.
: PS I would advise against the use of the Sonopen as it has not been specifically designed for Spotweld Testing and may lead to false interpretations
.



 
 Reply 
 
kaushal ajudia
kaushal ajudia
06:03 Mar-12-2002
Re: Ultrasonic Testing of spot welds
hello everybody,


i need some informatin regarding the detailed working of ultrasonic testing for welds and in which way it is advantageous than other similar process.

please try to reply me on the above email address without fail if anyone can do so.


thanking you.



 
 Reply 
 
santosh dengle
santosh dengle
08:39 Jun-01-2013
Re: Ultrasonic Testing of spot welds
In Reply to Rolf Diederichs at 00:07 Aug-19-1999 .

We are leading Automobile manufacturer in India. We are interested in Ultrasonic testing of the spot welds for one of our product.
Pl. share more information including the technical & commercial aspects.
Also pl. confirm details of Indian company
Regards,
Santosh Dengle
Sr.Manager (Robotics & Automation)
Bajaj Auto Ltd.,Pune,India.

 
 Reply 
 
Sudheer Jai Krishnan
Sudheer Jai Krishnan
16:31 Jun-01-2013
Re: Ultrasonic Testing of spot welds
In Reply to santosh dengle at 08:39 Jun-01-2013 .

Hi Santosh

Epoch 600 or Epoch XT with appropriate transducers shall be the right option for you. Olympus has already supplied many Epoch's in the past to the automobile manufacturers in India and globally.

You shall contact srinjay.gogia@olympus.in

Regards

Sudheer Jai Krishnan

 
 Reply 
 
massimo carminati
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

massimo carminati

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
19:28 Jun-02-2013
Re: Ultrasonic Testing of spot welds
In Reply to santosh dengle at 08:39 Jun-01-2013 .

Make sure you have an appropriate pulser and receiver to drive correctly 20 to 25 MHz probes. There are some instruments with almost automatic evaluation.

 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window