Dick Dobson
Dick Dobson
06:22 Aug-27-1999
Testing for defects

Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
Thank you for your help.
Dick Dobson, Systems Engineer
www.conleyfrp.com

Conley Corporation
2795 East 91st Street
Tulsa, Oklahoma USA 74137
1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
07:15 Aug-27-1999
Re: Testing for defects

: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?

If your process can accomodate squirting water on the parts, you could use an on-line ultrasonic flaw detection system to find voids and delaminations. This is fairly straightforward for pipe testing. More complex shapes like fittings would require a contour-following scanner that would probably be too slow for 100% in-process inspection. (The limitation is that a focused sound beam has to be aimed at a specific angle wih respect to each point on the surface, so scanning complex shapes requires a lot of probe manipulation.)

My company is one of a number that make this sort of thing. You can find product information under the Automated Systems section of our web site.

--Tom Nelligan
Panametrics, Inc.
www.panametrics.com/ndt/


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
02:13 Aug-27-1999
Re: Testing for defects
: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
: Thank you for your help.

Dear Dick,

Lixi can offer to you either a hand held real time X-Ray (fluoroscope) or density profiler to find voids and variation in the density of the pipe.


Regards,

Joe Pascente
: Dick Dobson, Systems Engineer
: www.conleyfrp.com
:
: Conley Corporation
: 2795 East 91st Street
: Tulsa, Oklahoma USA 74137
: 1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907




 
 Reply 
 
Terry Oldberg
Engineering, Mechanical Electrical Nuclear Software
Consultant, USA, Joined Oct 1999, 42

Terry Oldberg

Engineering, Mechanical Electrical Nuclear Software
Consultant,
USA,
Joined Oct 1999
42
04:00 Aug-31-1999
Re: Testing for defects
: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
: Thank you for your help.
: Dick Dobson, Systems Engineer
: www.conleyfrp.com
:
: Conley Corporation
: 2795 East 91st Street
: Tulsa, Oklahoma USA 74137
: 1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907




 
 Reply 
 
Terry Oldberg
Engineering, Mechanical Electrical Nuclear Software
Consultant, USA, Joined Oct 1999, 42

Terry Oldberg

Engineering, Mechanical Electrical Nuclear Software
Consultant,
USA,
Joined Oct 1999
42
06:30 Aug-31-1999
Re: Testing for defects
I recommend that you restate your requirement, as all of the various tests for defects are partially or completely opaque to scientific investigation. For information on this, see the discussion of violations of the Unit Measure axiom of probability theory in this forum. To give yourself the basis for evaluating bids, ask the bidders to supply you with the false negative and false positive error probabilities for the proposed tests.

Tests that are open to scientific investigation have the property of preserving the Unit Measure axiom of probability theory. To accomplish this, specify that the test is to classify each element of a partition of the material as sound or defective by reference to a definitive test which you name.

: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
: Thank you for your help.
: Dick Dobson, Systems Engineer
: www.conleyfrp.com
:
: Conley Corporation
: 2795 East 91st Street
: Tulsa, Oklahoma USA 74137
: 1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907




 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>