Testing for defects

Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
Thank you for your help.
Dick Dobson, Systems Engineer
www.conleyfrp.com

Conley Corporation
2795 East 91st Street
Tulsa, Oklahoma USA 74137
1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
07:15 Aug-27-1999
Re: Testing for defects

: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?

If your process can accomodate squirting water on the parts, you could use an on-line ultrasonic flaw detection system to find voids and delaminations. This is fairly straightforward for pipe testing. More complex shapes like fittings would require a contour-following scanner that would probably be too slow for 100% in-process inspection. (The limitation is that a focused sound beam has to be aimed at a specific angle wih respect to each point on the surface, so scanning complex shapes requires a lot of probe manipulation.)

My company is one of a number that make this sort of thing. You can find product information under the Automated Systems section of our web site.

--Tom Nelligan
Panametrics, Inc.
www.panametrics.com/ndt/


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
02:13 Aug-27-1999
Re: Testing for defects
: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
: Thank you for your help.

Dear Dick,

Lixi can offer to you either a hand held real time X-Ray (fluoroscope) or density profiler to find voids and variation in the density of the pipe.


Regards,

Joe Pascente
: Dick Dobson, Systems Engineer
: www.conleyfrp.com
:
: Conley Corporation
: 2795 East 91st Street
: Tulsa, Oklahoma USA 74137
: 1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907




 
 Reply 
 
Terry Oldberg
Engineering, Mechanical Electrical Nuclear Software
Consultant, USA, Joined Oct 1999, 42

Terry Oldberg

Engineering, Mechanical Electrical Nuclear Software
Consultant,
USA,
Joined Oct 1999
42
04:00 Aug-31-1999
Re: Testing for defects
: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
: Thank you for your help.
: Dick Dobson, Systems Engineer
: www.conleyfrp.com
:
: Conley Corporation
: 2795 East 91st Street
: Tulsa, Oklahoma USA 74137
: 1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907




 
 Reply 
 
Terry Oldberg
Engineering, Mechanical Electrical Nuclear Software
Consultant, USA, Joined Oct 1999, 42

Terry Oldberg

Engineering, Mechanical Electrical Nuclear Software
Consultant,
USA,
Joined Oct 1999
42
06:30 Aug-31-1999
Re: Testing for defects
I recommend that you restate your requirement, as all of the various tests for defects are partially or completely opaque to scientific investigation. For information on this, see the discussion of violations of the Unit Measure axiom of probability theory in this forum. To give yourself the basis for evaluating bids, ask the bidders to supply you with the false negative and false positive error probabilities for the proposed tests.

Tests that are open to scientific investigation have the property of preserving the Unit Measure axiom of probability theory. To accomplish this, specify that the test is to classify each element of a partition of the material as sound or defective by reference to a definitive test which you name.

: Conley Corporation is a manufacturer of corrosion resistant nexus reinforced filament wound fiberglass pipe and fittings, double containment fiberglass reinforced pipe and fittings, valves and strainers, and complete frp piping systems.
: Do you know of any online (production) testing equipment or systems for detecting flaws, laminations, voids, etc. in the production of filament wound pipes and fittings?
: Thank you for your help.
: Dick Dobson, Systems Engineer
: www.conleyfrp.com
:
: Conley Corporation
: 2795 East 91st Street
: Tulsa, Oklahoma USA 74137
: 1-800-331-5502 or (918) 299-5051 / Fax (918) 299-5907




 
 Reply 
 

Product Spotlight

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window