Azhar
Azhar
02:48 Feb-04-2007
Ask

How to carried out Ultrasonic Inspection on two layers material


 
 Reply 
 
Nigel
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
05:56 Feb-04-2007
Re: Ask
Azhar

Your question is too vague to allow a reasonable response. Which materials, relative thicknesses, bonding or joining method, what type and size of indications are you looking for? More details and you will probably get a response.


----------- Start Original Message -----------
: How to carried out Ultrasonic Inspection on two layers material
------------ End Original Message ------------




 
 Reply 
 
AZHAR
AZHAR
02:30 Feb-07-2007
Re: Ask
thanks for you respons nigel,


actually i just need to know,how we can carried out UT on two material with different properties.can you give the idea?,i means that what technique we have to used


 
 Reply 
 
Ed D.
Ed D.
06:06 Feb-07-2007
Re: Ask
----------- Start Original Message -----------
: thanks for you respons nigel,
:
: actually i just need to know,how we can carried out UT on two material with different properties.can you give the idea?,i means that what technique we have to used
------------ End Original Message ------------

WHat kind of differences are you taking about? Yu are being very vague.
If you mean velocity differences then you need to use a different calibraiton block for each material.



 
 Reply 
 
Nigel
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
08:17 Feb-07-2007
Re: Ask
If its a bonded joint then I suggest you have a test block made of the two materials with an intentional disbond area equivalent in size to the smallest area you wish to detect. Then, using a suitable compression wave probe, you can compare the response from the actual disbond with the reflection occasioned by the different acoustic impedances of the two materials according to the formula given on this page:

http://www.ndt.net/article/az/ut/reflc.htm

Very general I know but you are not giving any details of the test item. Use the excellent UT encyclopaedia on here.





 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1303

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1303
02:37 Feb-07-2007
Re: Ask
Azhar:
You have still not provided any details of your problem.
Might I suggest that as a starter you could simply use Nigel's list of items as a checklist and provide the details he itemised:
e.g.
Which materials: carbon steel to stainless

relative thicknesses: 3mm stainless to 25mm carbon steel

bonding or joining method: explosive welding

and so on....

Without information on the details no response is possible....There are some situations where ultrasonic testing may not be appropriate or perhaps even there are no NDT options available!
Ed

----------- Start Original Message -----------
: Azhar
: Your question is too vague to allow a reasonable response. Which materials, relative thicknesses, bonding or joining method, what type and size of indications are you looking for? More details and you will probably get a response.
:
: : How to carried out Ultrasonic Inspection on two layers material
------------ End Original Message ------------




 
 Reply 
 
Ed D.
Ed D.
05:49 Feb-08-2007
Re: Ask
----------- Start Original Message -----------
: Azhar:
: You have still not provided any details of your problem.
: Might I suggest that as a starter you could simply use Nigel's list of items as a checklist and provide the details he itemised:
: e.g.
: Which materials: carbon steel to stainless
: relative thicknesses: 3mm stainless to 25mm carbon steel
: bonding or joining method: explosive welding
: and so on....
: Without information on the details no response is possible....There are some situations where ultrasonic testing may not be appropriate or perhaps even there are no NDT options available!
: Ed
:
: : Azhar
: : Your question is too vague to allow a reasonable response. Which materials, relative thicknesses, bonding or joining method, what type and size of indications are you looking for? More details and you will probably get a response.
: :
: : : How to carried out Ultrasonic Inspection on two layers material
------------ End Original Message ------------

I agree with Ed G. The bottom line however, is you will probabl;y need a calibraiton block for each material or as Ed stated a mock up


 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window