Penentrant materials

I find nothing in the ASTM 1417 spec. that covers the following issue.
When large tanks of penetrant are used to apply penetrant by dipping, when the tank level drops to a point that more penetrant is needed to bring the level up, if the new quantity of penetrant to be added is a different batch number, but the same manufacture and qualified to the same specifications, is it permissible to mix the new batch number with the existing batch?



 
 Reply 
 
Nigel
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
08:26 Feb-07-2007
Re: Penentrant materials
Dave

Dave

I cannot imagine anyone with any financial sense saying otherwise if the tank is depleted through carry over and the present material exceeds all the quality requirements. If you have a large tank presumably you have large items for immersion so the tank must be kept topped up. Keep a record of the how much was added and when. Just ensure you keep sufficient unused penetrant of the previous batch to be able to produce an unused mixture of the two batch numbers at the same proportions as in the tank as a control sample.

If the tank is at a low level it is an opportunity to drain off the penetrant to clean cans and clean out the bottom of the tank prior to replenishment.

Regards

Nigel


----------- Start Original Message -----------
: I find nothing in the ASTM 1417 spec. that covers the following issue.
: When large tanks of penetrant are used to apply penetrant by dipping, when the tank level drops to a point that more penetrant is needed to bring the level up, if the new quantity of penetrant to be added is a different batch number, but the same manufacture and qualified to the same specifications, is it permissible to mix the new batch number with the existing batch?
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window