Technical Discussions
azri
azri
05:39 Feb-11-2007
MPI Underwater

Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.

thank you


 
 Reply 
 
giorgio lucido
giorgio lucido
04:54 Feb-21-2007
Re: MPI Underwater
There are several UT single point measurement techniques and products for single point measurement (Cygnus for example).
also there is a Guided wave (LRUT) technique called GUL Subsea system for underwater inspection of long lengths of pipes.


 
 Reply 
 
Martin Lugg
Consultant,
Eddyfi Technologies, United Kingdom, Joined Nov 2000, 27

Martin Lugg

Consultant,
Eddyfi Technologies,
United Kingdom,
Joined Nov 2000
27
06:13 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.


 
 Reply 
 
Simon Amallraja
Director
PET Aviation Systems P Ltd, India, Joined Jul 2003, 20

Simon Amallraja

Director
PET Aviation Systems P Ltd,
India,
Joined Jul 2003
20
07:51 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: : Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: : thank you
: If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.
------------ End Original Message ------------

You can contact Force Technology from Denmark. They have sub sea UT application system mainly used for Off Shore drilling projects. www.forcetechnology.com will give more info for you.

Simon Amallraja


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
01:36 Feb-27-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

NEWT International has an excellent lightweight system for underwater inspection, which has displaced MPI for defect detection and sizing. The system is very portable. It doesn't use a high voltage AC supply in the umbilical as it was designed to use only a single twisted pair in an umbilical, which can be on a ROV, in a diver's umbilical or a separate lightweight cable.

We would be happy to give you some references.



 
 Reply 
 

Product Spotlight

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window