MPI Underwater

Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.

thank you


 
 Reply 
 
giorgio lucido
giorgio lucido
04:54 Feb-21-2007
Re: MPI Underwater
There are several UT single point measurement techniques and products for single point measurement (Cygnus for example).
also there is a Guided wave (LRUT) technique called GUL Subsea system for underwater inspection of long lengths of pipes.


 
 Reply 
 
Martin Lugg
Consultant,
Eddyfi Technologies, United Kingdom, Joined Nov 2000, 27

Martin Lugg

Consultant,
Eddyfi Technologies,
United Kingdom,
Joined Nov 2000
27
06:13 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.


 
 Reply 
 
Simon Amallraja
Director
PET Aviation Systems P Ltd, India, Joined Jul 2003, 20

Simon Amallraja

Director
PET Aviation Systems P Ltd,
India,
Joined Jul 2003
20
07:51 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: : Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: : thank you
: If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.
------------ End Original Message ------------

You can contact Force Technology from Denmark. They have sub sea UT application system mainly used for Off Shore drilling projects. www.forcetechnology.com will give more info for you.

Simon Amallraja


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
01:36 Feb-27-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

NEWT International has an excellent lightweight system for underwater inspection, which has displaced MPI for defect detection and sizing. The system is very portable. It doesn't use a high voltage AC supply in the umbilical as it was designed to use only a single twisted pair in an umbilical, which can be on a ROV, in a diver's umbilical or a separate lightweight cable.

We would be happy to give you some references.



 
 Reply 
 

Product Spotlight

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window