azri
05:39 Feb-11-2007
MPI Underwater

Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.

thank you


 
 Reply 
 
giorgio lucido
giorgio lucido
04:54 Feb-21-2007
Re: MPI Underwater
There are several UT single point measurement techniques and products for single point measurement (Cygnus for example).
also there is a Guided wave (LRUT) technique called GUL Subsea system for underwater inspection of long lengths of pipes.


 
 Reply 
 
Martin Lugg
Consultant,
Eddyfi Technologies, United Kingdom, Joined Nov 2000, 27

Martin Lugg

Consultant,
Eddyfi Technologies,
United Kingdom,
Joined Nov 2000
27
06:13 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.


 
 Reply 
 
Simon Amallraja
Director
PET Aviation Systems P Ltd, India, Joined Jul 2003, 20

Simon Amallraja

Director
PET Aviation Systems P Ltd,
India,
Joined Jul 2003
20
07:51 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: : Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: : thank you
: If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.
------------ End Original Message ------------

You can contact Force Technology from Denmark. They have sub sea UT application system mainly used for Off Shore drilling projects. www.forcetechnology.com will give more info for you.

Simon Amallraja


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
01:36 Feb-27-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

NEWT International has an excellent lightweight system for underwater inspection, which has displaced MPI for defect detection and sizing. The system is very portable. It doesn't use a high voltage AC supply in the umbilical as it was designed to use only a single twisted pair in an umbilical, which can be on a ROV, in a diver's umbilical or a separate lightweight cable.

We would be happy to give you some references.



 
 Reply 
 

Product Spotlight

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window