MPI Underwater

Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.

thank you


 
 Reply 
 
giorgio lucido
giorgio lucido
04:54 Feb-21-2007
Re: MPI Underwater
There are several UT single point measurement techniques and products for single point measurement (Cygnus for example).
also there is a Guided wave (LRUT) technique called GUL Subsea system for underwater inspection of long lengths of pipes.


 
 Reply 
 
Martin Lugg
Consultant,
Eddyfi Technologies, United Kingdom, Joined Nov 2000, 27

Martin Lugg

Consultant,
Eddyfi Technologies,
United Kingdom,
Joined Nov 2000
27
06:13 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.


 
 Reply 
 
Simon Amallraja
Director
PET Aviation Systems P Ltd, India, Joined Jul 2003, 20

Simon Amallraja

Director
PET Aviation Systems P Ltd,
India,
Joined Jul 2003
20
07:51 Feb-22-2007
Re: MPI Underwater
----------- Start Original Message -----------
: : Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: : thank you
: If you are looking at MPI underwater, you should consider ACFM. This was developed for inspecting welded tubular structures underwater and has several advantages for detecting surface-breaking defects: it can be used 24 hours per day, it provides defect depth information, it provides auditable results and doesn't rely on operator interpretation, and it doesn't require cleaning to bright metal.
------------ End Original Message ------------

You can contact Force Technology from Denmark. They have sub sea UT application system mainly used for Off Shore drilling projects. www.forcetechnology.com will give more info for you.

Simon Amallraja


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
01:36 Feb-27-2007
Re: MPI Underwater
----------- Start Original Message -----------
: Does anybody could give some knowledge of how to carried out UT and MPI for underwater, i means that the technique used and equipment used.
: thank you
------------ End Original Message ------------

NEWT International has an excellent lightweight system for underwater inspection, which has displaced MPI for defect detection and sizing. The system is very portable. It doesn't use a high voltage AC supply in the umbilical as it was designed to use only a single twisted pair in an umbilical, which can be on a ROV, in a diver's umbilical or a separate lightweight cable.

We would be happy to give you some references.



 
 Reply 
 

Product Spotlight

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window