where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

1061 views
Technical Discussions
Ben Bradley
Ben Bradley
00:33 Mar-01-2007
Corrosion thickness measurement

I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
04:45 Mar-01-2007
Re: Corrosion thickness measurement
There are many, many companies in that market, including mine. Here's a link to a detailed application note on the subject of ultrasonic corrosion gaging that includes links to data sheets on the various gages available in the Panametrics-NDT line from Olympus NDT.

----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:03 Mar-06-2007
Re: Corrosion thickness measurement
----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------

If you are looking for point measurement, you can use Corrosion Gages. You can look into Panametrics, Sonatest, KK, Danatronics etc and many more.

If you are looking for continuous mapping with data verification, speed and analysis, manufacturer's like NDT Solutions, Force Technology will help you.

You need to give more details to recommend suitable products for your application.

D.Simon Amallraja.


 
 Reply 
 
AGUSTIN JIMENEZ
AGUSTIN JIMENEZ
06:00 Mar-07-2007
Re: Corrosion thickness measurement
I RECOMMEND THE DMS 2 B-SCAN WITH PROBE HT 450WT OR FH2E.
I HAVE USED IT EQUIPMENT MANY TIME IS VERY EFFECTIVE.

----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 
Phil Thayer
Phil Thayer
07:17 Mar-07-2007
Re: Corrosion thickness measurement
Please go to ndtautomation.com. We have released the Pocket UT, hand held A,B and C-Scan system. Will perform a B-scan for corrossion mapping. Weighs less then 2 pounds. Compatible with most all encoded scans and can even control 2 axis motorized scanners. Should be perfect for your application.

Phil Thayer
609-716-4051

----------- Start Original Message -----------
: I RECOMMEND THE DMS 2 B-SCAN WITH PROBE HT 450WT OR FH2E.
: I HAVE USED IT EQUIPMENT MANY TIME IS VERY EFFECTIVE.
: : I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Portable Ground Penetrating Radar - Proceq GP8000

The Proceq GP8000 portable ground penetrating radar instrument is the beginning of a new era in ND
...
T. The outstanding, patented ultra- wideband technology combined with a compact wireless probe delivers unmatched industry performance. Proceq GP8000 is the world’s first large-scale inspection solution that utilizes Augmented Reality in industrial applications.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>