Ben Bradley
Ben Bradley
00:33 Mar-01-2007
Corrosion thickness measurement

I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
04:45 Mar-01-2007
Re: Corrosion thickness measurement
There are many, many companies in that market, including mine. Here's a link to a detailed application note on the subject of ultrasonic corrosion gaging that includes links to data sheets on the various gages available in the Panametrics-NDT line from Olympus NDT.

----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:03 Mar-06-2007
Re: Corrosion thickness measurement
----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------

If you are looking for point measurement, you can use Corrosion Gages. You can look into Panametrics, Sonatest, KK, Danatronics etc and many more.

If you are looking for continuous mapping with data verification, speed and analysis, manufacturer's like NDT Solutions, Force Technology will help you.

You need to give more details to recommend suitable products for your application.

D.Simon Amallraja.


 
 Reply 
 
AGUSTIN JIMENEZ
AGUSTIN JIMENEZ
06:00 Mar-07-2007
Re: Corrosion thickness measurement
I RECOMMEND THE DMS 2 B-SCAN WITH PROBE HT 450WT OR FH2E.
I HAVE USED IT EQUIPMENT MANY TIME IS VERY EFFECTIVE.

----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 
Phil Thayer
Phil Thayer
07:17 Mar-07-2007
Re: Corrosion thickness measurement
Please go to ndtautomation.com. We have released the Pocket UT, hand held A,B and C-Scan system. Will perform a B-scan for corrossion mapping. Weighs less then 2 pounds. Compatible with most all encoded scans and can even control 2 axis motorized scanners. Should be perfect for your application.

Phil Thayer
609-716-4051

----------- Start Original Message -----------
: I RECOMMEND THE DMS 2 B-SCAN WITH PROBE HT 450WT OR FH2E.
: I HAVE USED IT EQUIPMENT MANY TIME IS VERY EFFECTIVE.
: : I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window