Corrosion thickness measurement

I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
04:45 Mar-01-2007
Re: Corrosion thickness measurement
There are many, many companies in that market, including mine. Here's a link to a detailed application note on the subject of ultrasonic corrosion gaging that includes links to data sheets on the various gages available in the Panametrics-NDT line from Olympus NDT.

----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:03 Mar-06-2007
Re: Corrosion thickness measurement
----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------

If you are looking for point measurement, you can use Corrosion Gages. You can look into Panametrics, Sonatest, KK, Danatronics etc and many more.

If you are looking for continuous mapping with data verification, speed and analysis, manufacturer's like NDT Solutions, Force Technology will help you.

You need to give more details to recommend suitable products for your application.

D.Simon Amallraja.


 
 Reply 
 
AGUSTIN JIMENEZ
AGUSTIN JIMENEZ
06:00 Mar-07-2007
Re: Corrosion thickness measurement
I RECOMMEND THE DMS 2 B-SCAN WITH PROBE HT 450WT OR FH2E.
I HAVE USED IT EQUIPMENT MANY TIME IS VERY EFFECTIVE.

----------- Start Original Message -----------
: I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 
Phil Thayer
Phil Thayer
07:17 Mar-07-2007
Re: Corrosion thickness measurement
Please go to ndtautomation.com. We have released the Pocket UT, hand held A,B and C-Scan system. Will perform a B-scan for corrossion mapping. Weighs less then 2 pounds. Compatible with most all encoded scans and can even control 2 axis motorized scanners. Should be perfect for your application.

Phil Thayer
609-716-4051

----------- Start Original Message -----------
: I RECOMMEND THE DMS 2 B-SCAN WITH PROBE HT 450WT OR FH2E.
: I HAVE USED IT EQUIPMENT MANY TIME IS VERY EFFECTIVE.
: : I am currently researching ultrasound instruments to be used for thickness measurement of corroded steel plate. I was wondering if anyone can recommend any particular instruments that are good at this application? Robustness, ease of use, repeatability and reliability are all very important in this case.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window