Justin Cavanagh
Justin Cavanagh
00:20 Apr-10-2007
UT of cast iron at elevated tempratures

Has anyone got any advise for thickness inspections of cast iron valve bodies at elevated temps 280 degrees for example ???


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
07:26 Apr-10-2007
Re: UT of cast iron at elevated tempratures
What is the maximum thickness that you need to measure? Generally, the best approach for that test would be to use a high temperature dual element transducers. Cast iron is grainy and produces a lot of scatter noise, but you should be able to measure more than 50 mm/2 inches at 2 MHz with an appropriate instrument.

Some general tips on high temperature ultrasonic testing can be found in the attached application note.

----------- Start Original Message -----------
: Has anyone got any advise for thickness inspections of cast iron valve bodies at elevated temps 280 degrees for example ???
------------ End Original Message ------------




 
 Reply 
 
Justin Cavanagh
Justin Cavanagh
03:44 Apr-10-2007
Re: UT of cast iron at elevated tempratures
The casting is about 50mm I have run a 2mhz probe over it when cold and found it effective. I was thinking that would be a good way to go sounds like I am on the right track. Will just have to buy a high temp probe.
Emat probes have also been sugested for this aplication.

----------- Start Original Message -----------
: What is the maximum thickness that you need to measure? Generally, the best approach for that test would be to use a high temperature dual element transducers. Cast iron is grainy and produces a lot of scatter noise, but you should be able to measure more than 50 mm/2 inches at 2 MHz with an appropriate instrument.
: Some general tips on high temperature ultrasonic testing can be found in the attached application note.
: : Has anyone got any advise for thickness inspections of cast iron valve bodies at elevated temps 280 degrees for example ???
------------ End Original Message ------------




 
 Reply 
 
Borja Lopez
Director
Innerspec Technologies, USA, Joined Jun 2002, 36

Borja Lopez

Director
Innerspec Technologies,
USA,
Joined Jun 2002
36
04:16 Apr-11-2007
Re: UT of cast iron at elevated tempratures
----------- Start Original Message -----------
: Has anyone got any advise for thickness inspections of cast iron valve bodies at elevated temps 280 degrees for example ???
------------ End Original Message ------------

This could be a good application for EMAT. Please visit our website for additional info www.innerspec.com


 
 Reply 
 
Massimo Carminati
Massimo Carminati
03:24 Apr-12-2007
Re: UT of cast iron at elevated tempratures
As an alternative to a dual element high temperature probe (a very good one is the d797 panametrics, but the temperature is critical). I've had excellent results using a 2MHz BB single element with a Vespel delay line with a proper delay.



 
 Reply 
 

Product Spotlight

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window