ET testing for long products

Does anybody know ET standards for examination of steel long products (es. round bars)?
Thanks
Paolo


 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:19 Mar-06-2007
Re: ET testing for long products
----------- Start Original Message -----------
: Does anybody know ET standards for examination of steel long products (es. round bars)?
: Thanks
: Paolo
------------ End Original Message ------------

Contact Mr. Phil Herman Jr @ www.phtool.com and you will get the answer.

Simon


 
 Reply 
 
Debdutta Mallik
Consultant,
Malaysia, Joined Jun 2005, 37

Debdutta Mallik

Consultant,
Malaysia,
Joined Jun 2005
37
04:22 Apr-18-2007
Eddy Current Testing for long products
Dear Paolo,
There must be a standard for acceptance criteria of for eddy current testing of your product.If it is a long product then it can be done by online system. What kind of system you have.
For eddy current generally transverse or longitudinal notches are followed for calibration.starting from 0.2 and onwards depending upon the requirement of the specification.I can provide you the information regarding online surface inspection of rails.
Dont hesitate to ask if any further information required.

Best Regards,

Debdutta Mallik


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 221

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
221
03:16 Apr-26-2007
Re: Eddy Current Testing for long products
Please see NEWT International's website. I'm sure we can help you.

----------- Start Original Message -----------
: Dear Paolo,
: There must be a standard for acceptance criteria of for eddy current testing of your product.If it is a long product then it can be done by online system. What kind of system you have.
: For eddy current generally transverse or longitudinal notches are followed for calibration.starting from 0.2 and onwards depending upon the requirement of the specification.I can provide you the information regarding online surface inspection of rails.
: Dont hesitate to ask if any further information required.
: Best Regards,
: Debdutta Mallik
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window