Lorenzo Digregorio
Consultant, AUT specialist
IMG Ultrasuoni Srl, Italy, Joined Apr 2007, 691

Lorenzo Digregorio

Consultant, AUT specialist
IMG Ultrasuoni Srl,
Italy,
Joined Apr 2007
691
00:44 Apr-04-2007
Code Case 2235 compliance

Somebody has developed a "videorecording" system able to record the GE PHASOR screeen in correlation with an encoder mounted on the PA probe. In other words, the encoder is used as a "trigger" for recording the screen display. They claim it is "CODE CASE 2235 COMPLIANT". What is the forum opinion?


 
 Reply 
 
Massimo Carminati , E-mail:
Massimo Carminati , E-mail:
06:24 Apr-16-2007
Re: Code Case 2235 compliance
I don't believe that when the ASME committee stated that "the ultrasonic examination shall be performed using a device employing automatic computer based data acquisition" included a "movie" of the instrument screen! In my opinion "data" are "digitized UT signals in unprocessed form" and not a VGA output!



 
 Reply 
 
RT. Jeyakumar , E-mail:
RT. Jeyakumar , E-mail:
04:45 Apr-19-2007
Re: Code Case 2235 compliance
Good day,

I dont think Phasor can give recorded Video presentation. It would be like this., recorded image of TOFD can be post processed for Interpretation in offline (after the test).

So, you can run the image of TOFD (D-Scan) along with A-scan. So it gives real time offline presentation.

With Warm Regards,

RT. Jeyakumar

----------- Start Original Message -----------
: Somebody has developed a "videorecording" system able to record the GE PHASOR screeen in correlation with an encoder mounted on the PA probe. In other words, the encoder is used as a "trigger" for recording the screen display. They claim it is "CODE CASE 2235 COMPLIANT". What is the forum opinion?
------------ End Original Message ------------




 
 Reply 
 
Massimo Carminati , E-mail:
Massimo Carminati , E-mail:
07:35 Apr-20-2007
Re: Code Case 2235 compliance
Does it really allow to perform TOFD inspection?


 
 Reply 
 
RT. Jeyakumar , E-mail:
RT. Jeyakumar , E-mail:
08:24 Apr-20-2007
Re: Code Case 2235 compliance
Good day,

I dont know. But you can check equipment's technical specification with BS 7706.

With Warm regards,

RT. Jeyakumar


-----
------ Start Original Message -----------
: Does it really allow to perform TOFD inspection?
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window