Paolo
NDT Inspector,
Acciaierie Valbruna, Italy, Joined Nov 2006, 7

Paolo

NDT Inspector,
Acciaierie Valbruna,
Italy,
Joined Nov 2006
7
04:56 Mar-01-2007
ET testing for long products

Does anybody know ET standards for examination of steel long products (es. round bars)?
Thanks
Paolo


 
 Reply 
 
Simon Amallraja
Simon Amallraja
09:19 Mar-06-2007
Re: ET testing for long products
----------- Start Original Message -----------
: Does anybody know ET standards for examination of steel long products (es. round bars)?
: Thanks
: Paolo
------------ End Original Message ------------

Contact Mr. Phil Herman Jr @ www.phtool.com and you will get the answer.

Simon


 
 Reply 
 
Debdutta Mallik
Consultant,
Malaysia, Joined Jun 2005, 37

Debdutta Mallik

Consultant,
Malaysia,
Joined Jun 2005
37
04:22 Apr-18-2007
Eddy Current Testing for long products
Dear Paolo,
There must be a standard for acceptance criteria of for eddy current testing of your product.If it is a long product then it can be done by online system. What kind of system you have.
For eddy current generally transverse or longitudinal notches are followed for calibration.starting from 0.2 and onwards depending upon the requirement of the specification.I can provide you the information regarding online surface inspection of rails.
Dont hesitate to ask if any further information required.

Best Regards,

Debdutta Mallik


 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 221

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
221
03:16 Apr-26-2007
Re: Eddy Current Testing for long products
Please see NEWT International's website. I'm sure we can help you.

----------- Start Original Message -----------
: Dear Paolo,
: There must be a standard for acceptance criteria of for eddy current testing of your product.If it is a long product then it can be done by online system. What kind of system you have.
: For eddy current generally transverse or longitudinal notches are followed for calibration.starting from 0.2 and onwards depending upon the requirement of the specification.I can provide you the information regarding online surface inspection of rails.
: Dont hesitate to ask if any further information required.
: Best Regards,
: Debdutta Mallik
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window