Inspection of earthquake damaged concrete

What methods are available for the inspection of concrete in use as bridge support columns structural pillars etc?

I have heard of UT thru transmission and ground penetrating radar but what thicknesses can be examined.

Kind Regards

Michael Trinidad


 
 Reply 
 
Doug Mendes
NDT Inspector, R & D
Imetrix Inc., USA, Joined Oct 1999, 7

Doug Mendes

NDT Inspector, R & D
Imetrix Inc.,
USA,
Joined Oct 1999
7
06:26 Oct-28-1999
Re: Inspection of earthquake damaged concrete
Michael there are many areas of interest in concrete inspection,aggregate(grain) size,rebar location, rebar corrosion,and internal or surface cracks just to name a few.
Since you mentioned bridges, rebar corrosion and cracks would most likely be your primary areas of interest along with corrosion detection of the rebar.

All of these items are important but if you add into the equation of your support columns being in water and then add the difference of salt vs. fresh water the outcome of your examinations will vary.
Since all of these variables could apply to you i'm limited to the amount of help I can provide.
There are many methods of concrete inspection available but thier effective depth is dependent on the condtion sought for in the concrete.I suggest you get more specific with your question.I hope I have been of some help to you.

: What methods are available for the inspection of concrete in use as bridge support columns structural pillars etc?

: I have heard of UT thru transmission and ground penetrating radar but what thicknesses can be examined.

: Kind Regards

: Michael Trinidad




 
 Reply 
 
Jean Paul van Cuyck
Director
A2MS, Applied Acoustics, Materials and Systems, France, Joined Nov 1998, 13

Jean Paul van Cuyck

Director
A2MS, Applied Acoustics, Materials and Systems,
France,
Joined Nov 1998
13
00:48 Oct-28-1999
Re: Inspection of earthquake damaged concrete
: What methods are available for the inspection of concrete in use as bridge support columns structural pillars etc?

: I have heard of UT thru transmission and ground penetrating radar but what thicknesses can be examined.

: Kind Regards

: Michael Trinidad

It's depend on the deafult you have to observe. UT in concrete needs low frequencies
use, that implie low résolution default.
Please tell us more


 
 Reply 
 
Michael Trinidad
Consultant,
LMATS Pty Ltd , Australia, Joined Jan 2003, 141

Michael Trinidad

Consultant,
LMATS Pty Ltd ,
Australia,
Joined Jan 2003
141
03:47 Nov-01-1999
Re: Inspection of earthquake damaged concrete
I am currently working in Taiwan where recently we have had major earthquakes with 1000's of buildings destroyed and damaged. The damaged buildings (and bridges) have some uncertainity regarding their structural integrity. To compound the problem it has be noticed that many of the collapsed structures had poor workmanship.

Therefore any NDT examination would have to detect both poor workmanship (voids, lack of aggregate, no rebar etc) and structural damage (laminations, cracking),

: : Kind Regards

: : Michael Trinidad




 
 Reply 
 

Product Spotlight

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>