09:02 Oct-28-1999
Inspection of earthquake damaged concrete

What methods are available for the inspection of concrete in use as bridge support columns structural pillars etc?

I have heard of UT thru transmission and ground penetrating radar but what thicknesses can be examined.

Kind Regards

Michael Trinidad


 
 Reply 
 
Doug Mendes
NDT Inspector, R & D
Imetrix Inc., USA, Joined Oct 1999, 7

Doug Mendes

NDT Inspector, R & D
Imetrix Inc.,
USA,
Joined Oct 1999
7
06:26 Oct-28-1999
Re: Inspection of earthquake damaged concrete
Michael there are many areas of interest in concrete inspection,aggregate(grain) size,rebar location, rebar corrosion,and internal or surface cracks just to name a few.
Since you mentioned bridges, rebar corrosion and cracks would most likely be your primary areas of interest along with corrosion detection of the rebar.

All of these items are important but if you add into the equation of your support columns being in water and then add the difference of salt vs. fresh water the outcome of your examinations will vary.
Since all of these variables could apply to you i'm limited to the amount of help I can provide.
There are many methods of concrete inspection available but thier effective depth is dependent on the condtion sought for in the concrete.I suggest you get more specific with your question.I hope I have been of some help to you.

: What methods are available for the inspection of concrete in use as bridge support columns structural pillars etc?

: I have heard of UT thru transmission and ground penetrating radar but what thicknesses can be examined.

: Kind Regards

: Michael Trinidad




 
 Reply 
 
Jean Paul van Cuyck
Director
A2MS, Applied Acoustics, Materials and Systems, France, Joined Nov 1998, 13

Jean Paul van Cuyck

Director
A2MS, Applied Acoustics, Materials and Systems,
France,
Joined Nov 1998
13
00:48 Oct-28-1999
Re: Inspection of earthquake damaged concrete
: What methods are available for the inspection of concrete in use as bridge support columns structural pillars etc?

: I have heard of UT thru transmission and ground penetrating radar but what thicknesses can be examined.

: Kind Regards

: Michael Trinidad

It's depend on the deafult you have to observe. UT in concrete needs low frequencies
use, that implie low résolution default.
Please tell us more


 
 Reply 
 
Michael Trinidad
Consultant,
LMATS Pty Ltd , Australia, Joined Jan 2003, 141

Michael Trinidad

Consultant,
LMATS Pty Ltd ,
Australia,
Joined Jan 2003
141
03:47 Nov-01-1999
Re: Inspection of earthquake damaged concrete
I am currently working in Taiwan where recently we have had major earthquakes with 1000's of buildings destroyed and damaged. The damaged buildings (and bridges) have some uncertainity regarding their structural integrity. To compound the problem it has be noticed that many of the collapsed structures had poor workmanship.

Therefore any NDT examination would have to detect both poor workmanship (voids, lack of aggregate, no rebar etc) and structural damage (laminations, cracking),

: : Kind Regards

: : Michael Trinidad




 
 Reply 
 

Product Spotlight

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>