resin content monitoring in prepregs

Hi all,

We develop industrial low energy X-ray method and apparatus for monitoring of resin content in prepregs during production. Can anybody give us his thoughts about this method or show us a link where a X-ray method is used at presence in prepregs manufacturing?

Any thoughts will be greatly appreciated

Sincerelly,
Dr. Nikitin




 
 Reply 
 
John Brunk
Engineering, NDT Level III
Self employed, part-time, USA, Joined Oct 1999, 162

John Brunk

Engineering, NDT Level III
Self employed, part-time,
USA,
Joined Oct 1999
162
00:33 Jun-10-2007
Re: resin content monitoring in prepregs
----------- Start Original Message -----------
: Hi all,
: We develop industrial low energy X-ray method and apparatus for monitoring of resin content in prepregs during production. Can anybody give us his thoughts about this method or show us a link where a X-ray method is used at presence in prepregs manufacturing?
: Any thoughts will be greatly appreciated
: Sincerelly,
: Dr. Nikitin
------------ End Original Message ------------
You should take a careful look at the attenuation coefficients of the materials involved. X-ray may not be the best method for distinguishing graphite from the resin. Looking for actual voids is a different matter. Air-transmission ultrasound would be worth consideration.

John Brunk


 
 Reply 
 

Product Spotlight

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Content on Demand by Eddyfi Technologies

Finding yourself in front of a screen practicing safe social distancing instead of out in the fiel
...
d? At Eddyfi Technologies, we are doing our part in helping you be better prepared for what comes next. We introduce to you Eddyfi on Demand. Fill your schedule with webinars, how-to videos, informative technical papers and our NEW addition: Eddyfi Academy. There, you will have access to FREE online courses and obtain certificates of attendance once completed in order for you to include these e-learning sessions in your log of required training hours. Join us today. Stay safe, stay Beyond Current.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window