EN Welding Quality Standard

Good Day everyone,

A client wishes to qualify welders to EN 287-1:2004.

What is the current EN version of ISO 5817:2003?

My searches have only shown EN 25817:1993 as "superseded".
Is it correct to inspect to the ISO, or have changes been made to adopt as an EN?

Regards
Nick


    
 
 
ovidiu
NDT Inspector, thermography
ISCIR, Romania, Joined Dec 2005, 16

ovidiu

NDT Inspector, thermography
ISCIR,
Romania,
Joined Dec 2005
16
07:18 Jun-22-2007
Re: EN Welding Quality Standard
EN ISO 5817:2003 is in use

-----------Start Original Message -----------
: Good Day everyone,
: A client wishes to qualify welders to EN 287-1:2004.
: What is the current EN version of ISO 5817:2003?
: My searches have only shown EN 25817:1993 as "superseded".
: Is it correct to inspect to the ISO, or have changes been made to adopt as an EN?
: Regards
: Nick
------------ End Original Message ------------




    
 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 176

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
176
08:12 Jun-22-2007
Re: EN Welding Quality Standard
reply:

The actual documents are:

EN 287-1:2004 + Amendment 2:2006.

EN 25718 is superseded by a single EN ISO standard:

EN ISO 5817:2003 + Corrigendum 2006

Best regards

Udo Schlengermann
GE Inspection Technologies GmbH, Huerth, Germany
Convener CEN/TC121/SC5/WG2 (UT of welds)


----------- Start Original Message -----------
: Good Day everyone,
: A client wishes to qualify welders to EN 287-1:2004.
: What is the current EN version of ISO 5817:2003?
: My searches have only shown EN 25817:1993 as "superseded".
: Is it correct to inspect to the ISO, or have changes been made to adopt as an EN?
: Regards
: Nick
------------ End Original Message ------------




    
 
 

Product Spotlight

FlexoFORM™

The FlexoFORM™ solution integrates flexible phased array probe technology in a scanner to solv
...
e the challenges that come with inspecting pipe elbows. When combined with a water column, this solution can be used to collect easy-to-interpret data on elbows with diameters ranging from 4.5 in. OD up to flat and offers many benefits.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window