Technical Discussions
Mike
Mike
07:40 Jul-09-2007
Intrinsically Safe UT Methods

Currently, I am searching the market for a UT technique that is intrinsically safe to UK zone 1 or USA DIV 0 - 1. It appears the NDT manufacturing market does not offer such solution. Can anyone offer information to support an important market requirement.


 
 Reply 
 
Sunil Ramchandran
Sunil Ramchandran
09:12 Jul-09-2007
Re: Intrinsically Safe UT Methods
We have had clients with the same request/requirement.

My research failed to find any UT instrument manufacturers who make such an intrinsically safe machine.

If I recall correctly, either Panametrics or KB had made one for a few years, but the cost was prohibitive and the unit did not sell very well. Therefore, it was discontinued.

I would be interested to know if anyone has more information on this topic.

Great post, Mike.

Thanks.


 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
01:25 Jul-09-2007
Re: Intrinsically Safe UT Methods
Hi,

The only IS rated instrument I have run across is a D-meter from Cygnus instruments. Doesn't do shearwave, not very good for specialized corrosion applications due to it's single crystal design.

http://www.cygnus-instruments.com/launch.htm

Cygnus 1 IS

Cheers,

David Hermanutz

----------- Start Original Message -----------
: We have had clients with the same request/requirement.
: My research failed to find any UT instrument manufacturers who make such an intrinsically safe machine.
: If I recall correctly, either Panametrics or KB had made one for a few years, but the cost was prohibitive and the unit did not sell very well. Therefore, it was discontinued.
: I would be interested to know if anyone has more information on this topic.
: Great post, Mike.
: Thanks.
------------ End Original Message ------------




 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 158

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
158
01:33 Jul-10-2007
Re: Intrinsically Safe UT Methods
Hello Mike,
There is a Krautkramer brand ultrasonic flaw detector, the USM 23ex that is classed intrinsically safe to EN 50014 & 50020. See the link below for more info. If you have any further questions please do not to hesitate your local GE IT Krautkramer ultrasonics distributor.
Regards

Neil Burleigh
----------- Start Original Message -----------
: Currently, I am searching the market for a UT technique that is intrinsically safe to UK zone 1 or USA DIV 0 - 1. It appears the NDT manufacturing market does not offer such solution. Can anyone offer information to support an important market requirement.
------------ End Original Message ------------




 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 158

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
158
01:35 Jul-10-2007
Re: Intrinsically Safe UT Methods
----------- Start Original Message -----------
: Hello Mike,
: There is a Krautkramer brand ultrasonic flaw detector, the USM 23ex that is classed intrinsically safe to EN 50014 & 50020. See the link below for more info. If you have any further questions please do not to hesitate your local GE IT Krautkramer ultrasonics distributor.
: Regards
: Neil Burleigh
PS I am not sure if the link went with the post so I will include it in the body of the text.
http://www.geinspectiontechnologies.com/download/products/ut/fd/GEIT-20004-p-GB_usm23ex.pdf
: : Currently, I am searching the market for a UT technique that is intrinsically safe to UK zone 1 or USA DIV 0 - 1. It appears the NDT manufacturing market does not offer such solution. Can anyone offer information to support an important market requirement.
------------ End Original Message ------------




 
 Reply 
 
Joe
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 526

Joe

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
526
02:58 Jul-10-2007
Re: Intrinsically Safe UT Methods
The problem is not the Flaw detector as such, but the fact that customers are very inconsiderate and want to connect probes to it. This raises issues of sparking when disconnecting probes, cable damage etc.

The Cygnus IS thickness gauge is the only 'standard instrument' I'm aware of - This is relatively simple because the application uses a single probe - It doesn't need to be disconnectable.

KK used to make an explosion proof Flaw Detector the USM 23ex - Not sure if it is still available. as far as I know (I'm sure I'll be corrected if wrong) it had some limitations of low pulser voltage and limited probe options to maintain IS approval. But it was the only one around so gave you options you wouldn't have otherwise.

We (Sonatest) looked at producing one some years ago, but the technical issues, cost of certification, limited market and inherent limitations made us decide against it. It would be nice if we could produce an IS Flaw Detector with the same performance as a standard one, but its not an option, so generally we find operators prefer to live with the requirement for hot-work permits or whatever.

Good luck
Joe

----------- Start Original Message -----------
: Currently, I am searching the market for a UT technique that is intrinsically safe to UK zone 1 or USA DIV 0 - 1. It appears the NDT manufacturing market does not offer such solution. Can anyone offer information to support an important market requirement.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>