Mario J Santos
Teacher
Dep. Eng. Electrotecnica / U. Coimbra, Portugal, Joined Jan 2001, 1

Mario J Santos

Teacher
Dep. Eng. Electrotecnica / U. Coimbra,
Portugal,
Joined Jan 2001
1
06:21 Jan-26-2001
Ultrasonic paper testing


I am interested in study ultrasound propagation in paper by contact mode.

In the beginning I am interested only in the detection of the signal trough the paper (Lamb waves or similar) and velocity measurements in different directions.

I have knowledge of a commercial equipment for this propose that use bimorph ceramics.

I want to know if anybody knows a transducer for this application.


Best regards



 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
07:00 Jan-26-2001
Re: Ultrasonic paper testing
By using the forum search I could find two old forum topics that dealed with Ultrasonic paper testing.

measuring paper
http://www.ndt.net/wshop/forum/messages/71.htm

Contact transducers with paper??
http://www.ndt.net/wshop/forum/messages/190.htm


:
: I am interested in study ultrasound propagation in paper by contact mode.

: In the beginning I am interested only in the detection of the signal trough the paper (Lamb waves or similar) and velocity measurements in different directions.

: I have knowledge of a commercial equipment for this propose that use bimorph ceramics.

: I want to know if anybody knows a transducer for this application.

:
: Best regards




 
 Reply 
 
Rogerio
Rogerio
03:58 May-23-2001
Ultrasonic
:
: I am interested in study ultrasound aplication in pulp and paper.
: In the beginning I am interested only in the efects ultrasonic waves in cellulose fiber.
: I want to know if this application is possible
:
: Best regards




 
 Reply 
 
Rogerio
Rogerio
03:59 May-23-2001
Ultrasonic
:
: I am interested in study ultrasound aplication in pulp and paper.
: In the beginning I am interested only in the efects of ultrasonic waves in cellulose fiber.
: I want to know if this application is possible.
:
: Best regards




 
 Reply 
 
Rogerio
Rogerio
03:59 May-23-2001
Ultrasonic
:
: I am interested in study ultrasound aplication in pulp and paper.
: In the beginning I am interested only in the efects of ultrasonic waves in cellulose fiber.
: I want to know if this application is possible.
:
: Best regards




 
 Reply 
 
Williams Suinaga
Williams Suinaga
09:26 Nov-03-2001
Re: Ultrasonic
: :
: : I am interested in study ultrasound aplication in roal transports.
: : I want to know if this application is possible.
: :
: : Best regards
.



 
 Reply 
 
Manuel López
Manuel López
03:15 Aug-30-2002
Re: Ultrasonic paper bleaching and deinking
: : I'm looking for information about different deinking process.
: : I am interested in study ultrasound bleaching and deinking in paper.
.
: : please sent to me afew documants which I am interseted
: : Best regards
.



 
 Reply 
 

Product Spotlight

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Micro CT

nanoVoxel series has nano-scale resolution upto 500nm by using high voltage X-ray source (from 80-
...
300 kV) with micro/nano focal spot and highly sensitive flat panel detectors and unique Optical coupling detector.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window