ACS-Solutions GmbH
develop and manufacture hi-tech devices for Ultrasonic Testing
2006 views
Technical Discussions
Ing. Tomas Perez A.
NDT Inspector
Refineria Panama,S.A. (TEXACO), Algeria, Joined Dec 1999, 3

Ing. Tomas Perez A.

NDT Inspector
Refineria Panama,S.A. (TEXACO),
Algeria,
Joined Dec 1999
3
07:55 Nov-16-1999
Thickness measurement with coating.

I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
Thanks.



 
 Reply 
 
Wieslaw Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 265

Wieslaw Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
265
08:20 Nov-16-1999
Re: Thickness measurement with coating.
: I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
: Thanks.

Yes, it is possible, if you will measure from the other side of the wall.
You can use the same equipment, only the software must be able to measure and show the changes during the coating.

W. Bicz

http://www.optel.com.pl



 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
08:35 Nov-16-1999
Re: Thickness measurement with coating.

: I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
: Thanks.

What type of coating is this, and how thick is it? Is it solid or porous? Is it being applied at high temperature? If you can provide some further details of what you're trying to do, I may be able to suggest equipment and procedure.

--Tom Nelligan




 
 Reply 
 
Rod Martin
Sales,
NDT Equipment Sales Pty Limited, Australia, Joined Oct 1999, 10

Rod Martin

Sales,
NDT Equipment Sales Pty Limited,
Australia,
Joined Oct 1999
10
00:53 Nov-17-1999
Re: Thickness measurement with coating.

: I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
: Thanks.

Yes, it is possible to take readings of pipe wall thickness using the "Profiler". When a known wall thickness is calibrated, both wall loss or build-up can be read from a display graph used with the Profiler. For further information please forward your fax number to (61-2) 9524-0560.

Rod Martin
NDT EQUIPMENT SALES PTY LTD




 
 Reply 
 
Jean Paul van Cuyck
Director
A2MS, Applied Acoustics, Materials and Systems, France, Joined Nov 1998, 13

Jean Paul van Cuyck

Director
A2MS, Applied Acoustics, Materials and Systems,
France,
Joined Nov 1998
13
09:00 Nov-17-1999
Re: Thickness measurement with coating.
: I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
: Thanks.

Conceptually Yes. But you have to check the ultrasonics
frequency use with the coating thickness.

Please send a scheme with dimension and materials kind indicated.
I will think specifications to your system.

Fax nomber +33 491 828 494
email a2ms@agl.univ-mrs.fr
Confidentiality is guaranted



 
 Reply 
 
Schnitger, Christoph
Schnitger, Christoph
03:14 Nov-27-1999
Re: Thickness measurement with coating.
Hello ...

i have a used ultrasonic thicknessmeter for sale, called the Cygnus 1 , which is able to measure the
wall thickness through ( thin coating !)!!??

Please take a look, at my ONLINE SHOP for more information !



 
 Reply 
 
Jorge Lustosa
Jorge Lustosa
03:33 Jun-04-2000
Re: Steel thickness measurement
: Hello ...

: i have a used ultrasonic thicknessmeter for sale, called the Cygnus 1 , which is able to measure the
: wall thickness through paint coating . I would like to know price and availability for this equipment.
I also need Price and availability for Roxby MK V cathodic protection measurement equipment, as well as three Half cells ag/agcl.

: Please take a look, at my ONLINE SHOP for more information !




 
 Reply 
 
Majid Vahid
Majid Vahid
02:28 Aug-29-2001
Re: Thickness measurement with coating.
:What we need is a device to measure the thickness of paint .In the line of paint & resin.
Thanking you and best regards
M.Vahid
: : I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
: : Thanks.

: What type of coating is this, and how thick is it? Is it solid or porous? Is it being applied at high temperature? If you can provide some further details of what you're trying to do, I may be able to suggest equipment and procedure.

: --Tom Nelligan




 
 Reply 
 
Tom Carodiskey
Engineering
GE Inspection Technologies, USA, Joined Nov 1998, 1

Tom Carodiskey

Engineering
GE Inspection Technologies,
USA,
Joined Nov 1998
1
02:09 Aug-29-2001
Re: Thickness measurement with coating.
It it possible to measure both the coating thickness and the base metal thickness of heavily corroded pipe.
These measurements may be taken at the same time using a technique developed by Krautkramer. The TopCoat method utilizes multiple probes in a single housing to measure both the coating thickness and the total time of flight of the coating and the base metal. The corrected difference, of course, is the thickness of the base metal. This technique employs the normal high gain dual probe thickness measurment method that is widely used to measure accuratly to heavily corroded backwalls. There is no minimum coating thickness resolution issue with this technique. The Krautkramer DMS-2 has this capability.


: :What we need is a device to measure the thickness of paint .In the line of paint & resin.
: Thanking you and best regards
: M.Vahid
: : : I want to know, if is possible, to take readings of thicknesses in piping and plates where they are getting coating. What is the procedure, what are the UT equipment that I need?
: : : Thanks.
.
: : What type of coating is this, and how thick is it? Is it solid or porous? Is it being applied at high temperature? If you can provide some further details of what you're trying to do, I may be able to suggest equipment and procedure.
.
: : --Tom Nelligan
.



 
 Reply 
 

Product Spotlight

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window