Monitoring/Testing of fatigue in metals??

Could you please help me find current techniques (ultrasound; laboratory or field-use technique) used to monitor/test metals under conditions of repetitive use to determine risk of fatigue failure?

Thanks
Shreefal Mehta, Ph.D.
shreefal.mehta@email.swmed.edu


 
 Reply 
 
Liviu Singher
R & D,
Technion, Israel, Joined Nov 1998, 11

Liviu Singher

R & D,
Technion,
Israel,
Joined Nov 1998
11
02:41 Nov-21-1999
Re: Monitoring/Testing of fatigue in metals??



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
08:49 Nov-22-1999
Re: Monitoring/Testing of fatigue in metals??
: Could you please help me find current techniques (ultrasound; laboratory or field-use technique) used to monitor/test metals under conditions of repetitive use to determine risk of fatigue failure?

: Thanks
: Shreefal Mehta, Ph.D.
: shreefal.mehta@email.swmed.edu

Hi,
I ave been working with the "Resonant Fingerprint" method of condition monitoring for high value individually identifiable components.
In this method, the Resonant Fingerprint (either in the acoustic or ultrasonic range) is recorded when the component or structure is new or in known good condition, and again at regular periods or when the component has been subjected to a traumatic stress. Changes in the fingerprint signify changes in the structural integrity of the component.

Contact me for more details, or see Insight August 1988, pages 500 to 503.
Phone +44 24 7632 0812
Fax +44 24 7632 0813
email Godfrey@hands-ndt.co.uk
Godfrey Hands




 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
08:49 Nov-22-1999
Re: Monitoring/Testing of fatigue in metals??
: Could you please help me find current techniques (ultrasound; laboratory or field-use technique) used to monitor/test metals under conditions of repetitive use to determine risk of fatigue failure?

: Thanks
: Shreefal Mehta, Ph.D.
: shreefal.mehta@email.swmed.edu

Hi,
I have been working with the "Resonant Fingerprint" method of condition monitoring for high value individually identifiable components.
In this method, the Resonant Fingerprint (either in the acoustic or ultrasonic range) is recorded when the component or structure is new or in known good condition, and again at regular periods or when the component has been subjected to a traumatic stress. Changes in the fingerprint signify changes in the structural integrity of the component.

Contact me for more details, or see Insight August 1988, pages 500 to 503.
Phone +44 24 7632 0812
Fax +44 24 7632 0813
email Godfrey@hands-ndt.co.uk
Godfrey Hands




 
 Reply 
 
Jens Forker
Jens Forker
01:32 Dec-20-1999
Re: Monitoring/Testing of fatigue in metals??
: Could you please help me find current techniques (ultrasound; laboratory or field-use technique) used to monitor/test metals under conditions of repetitive use to determine risk of fatigue failure?

: Thanks
: Shreefal Mehta, Ph.D.
: shreefal.mehta@email.swmed.edu

Acoustic Emission testing (passive listening/detection to acoustic waves emitted when sudden material changes, e.g. crack growth, take place) is a method which can help. You can easily achieve integral monitoring of your sample and get online information.

for further information see our homepage www.vallen.de or contact me directly.
Jens Forker



 
 Reply 
 
sdf
sdf
07:44 Dec-01-2000
Re: Monitoring/Testing of fatigue in metals??
: : Could you please help me find current techniques (ultrasound; laboratory or field-use technique) used to monitor/test metals under conditions of repetitive use to determine risk of fatigue failure?

: : Thanks
: : Shreefal Mehta, Ph.D.
: : shreefal.mehta@email.swmed.edu

: Hi,
: I have been working with the "Resonant Fingerprint" method of condition monitoring for high value individually identifiable components.
: In this method, the Resonant Fingerprint (either in the acoustic or ultrasonic range) is recorded when the component or structure is new or in known good condition, and again at regular periods or when the component has been subjected to a traumatic stress. Changes in the fingerprint signify changes in the structural integrity of the component.

: Contact me for more details, or see Insight August 1988, pages 500 to 503.
: Phone +44 24 7632 0812
: Fax +44 24 7632 0813
: email Godfrey@hands-ndt.co.uk
: Godfrey Hands




 
 Reply 
 
H. N. Singh
H. N. Singh
01:49 Aug-12-2002
Re: Monitoring/Testing of fatigue in metals??
COuld u tell any method for evaluating fatigue life valuation using NDT method
: Thanks
: H N SIngh.
: hemnarain@rediffmail.com





 
 Reply 
 

Product Spotlight

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>