Tom
Tom
09:50 Aug-14-2007
Elliptical Shots

Does anyone know a general rule of thumb as to how much of an offset you should use to radiograph a 2" joint using an elliptical exposure?


 
 Reply 
 
Dent
Consultant, NDE Manager NDELevel III/3
NDT Consultant, Canada, Joined Nov 1998, 252

Dent

Consultant, NDE Manager NDELevel III/3
NDT Consultant,
Canada,
Joined Nov 1998
252
05:10 Aug-14-2007
Re: Elliptical Shots
----------- Start Original Message -----------
: Does anyone know a general rule of thumb as to how much of an offset you should use to radiograph a 2" joint using an elliptical exposure?
------------ End Original Message ------------

15 Deg should work.


 
 Reply 
 
DJ Kallhof
DJ Kallhof
08:38 Aug-14-2007
Re: Elliptical Shots
----------- Start Original Message -----------
: : Does anyone know a general rule of thumb as to how much of an offset you should use to radiograph a 2" joint using an elliptical exposure?
: 15 Deg should work.
------------ End Original Message ------------

7 : 1 ratio has worked well for me in the past. Back off 14" and offset 2" or 21" and offset 3". You get the idea. The only thing that can make it tricky is excessive weld build up of the root or crown. Take a technique and adjust accordingly.



 
 Reply 
 
chris s
chris s
00:44 Aug-15-2007
Re: Elliptical Shots
----------- Start Original Message -----------
: : : Does anyone know a general rule of thumb as to how much of an offset you should use to radiograph a 2" joint using an elliptical exposure?
: : 15 Deg should work.
: 7 : 1 ratio has worked well for me in the past. Back off 14" and offset 2" or 21" and offset 3". You get the idea. The only thing that can make it tricky is excessive weld build up of the root or crown. Take a technique and adjust accordingly.
------------ End Original Message ------------

i use the 7:1 ratio also, works fine. until you get into heavy wall


 
 Reply 
 
G.Madhesan
G.Madhesan
01:44 Aug-22-2007
Re: Elliptical Shots
As said by Mr.Dent You can use a 7:1 technique but you have to consider the thickness of the pipe because the root will vary deponds upon the wall thick.


 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window