NDT after PWHT

Dear All,

Pipe spool fabrication base on Code and standards B31.3.

Everyone can give to me advice ?

MT after PWHT shall be done or not necessary ?

Thanks and Best Regards,


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
08:38 Aug-24-2007
Re: NDT after PWHT

See B31.3 Para. 341.3.1.(a) "For P-Nos. 3, 4, and 5 materials, examination shall be performed after completion of any heat treatment."

This implies that P1 and P2 materials do not require examination after heat treatment UNLESS otherwise specified by the contract or relevant procedures.


 
 Reply 
 
G.Madhesan
G.Madhesan
08:29 Aug-24-2007
Re: NDT after PWHT
MT must be carriedout after any PWHT for detectingany stress cracks.
Regards,
Madhesan





 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
04:53 Aug-25-2007
Re: NDT after PWHT
Madhesan

Yes you are right MT, is for detecting cracks (amongst other defects), however the Code writers are very experienced in the welding and heat-treating of standard materials (i.e. Group P1) and are sufficiently confident that proper PWHT of such materials will not cause cracking to be able to codify this with no requirement for PWHT MT. So in the case of welding plain carbon (P1)steels, "must" does not apply.


----------- Start Original Message -----------
: MT must be carriedout after any PWHT for detectingany stress cracks.
: Regards,
: Madhesan
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window