NDT after PWHT

Dear All,

Pipe spool fabrication base on Code and standards B31.3.

Everyone can give to me advice ?

MT after PWHT shall be done or not necessary ?

Thanks and Best Regards,


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
08:38 Aug-24-2007
Re: NDT after PWHT

See B31.3 Para. 341.3.1.(a) "For P-Nos. 3, 4, and 5 materials, examination shall be performed after completion of any heat treatment."

This implies that P1 and P2 materials do not require examination after heat treatment UNLESS otherwise specified by the contract or relevant procedures.


 
 Reply 
 
G.Madhesan
G.Madhesan
08:29 Aug-24-2007
Re: NDT after PWHT
MT must be carriedout after any PWHT for detectingany stress cracks.
Regards,
Madhesan





 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
04:53 Aug-25-2007
Re: NDT after PWHT
Madhesan

Yes you are right MT, is for detecting cracks (amongst other defects), however the Code writers are very experienced in the welding and heat-treating of standard materials (i.e. Group P1) and are sufficiently confident that proper PWHT of such materials will not cause cracking to be able to codify this with no requirement for PWHT MT. So in the case of welding plain carbon (P1)steels, "must" does not apply.


----------- Start Original Message -----------
: MT must be carriedout after any PWHT for detectingany stress cracks.
: Regards,
: Madhesan
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window