Dear All,

Pipe spool fabrication base on Code and standards B31.3.

Everyone can give to me advice ?

MT after PWHT shall be done or not necessary ?

Thanks and Best Regards,


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
08:38 Aug-24-2007
Re: NDT after PWHT

See B31.3 Para. 341.3.1.(a) "For P-Nos. 3, 4, and 5 materials, examination shall be performed after completion of any heat treatment."

This implies that P1 and P2 materials do not require examination after heat treatment UNLESS otherwise specified by the contract or relevant procedures.


 
 Reply 
 
G.Madhesan
G.Madhesan
08:29 Aug-24-2007
Re: NDT after PWHT
MT must be carriedout after any PWHT for detectingany stress cracks.
Regards,
Madhesan





 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
04:53 Aug-25-2007
Re: NDT after PWHT
Madhesan

Yes you are right MT, is for detecting cracks (amongst other defects), however the Code writers are very experienced in the welding and heat-treating of standard materials (i.e. Group P1) and are sufficiently confident that proper PWHT of such materials will not cause cracking to be able to codify this with no requirement for PWHT MT. So in the case of welding plain carbon (P1)steels, "must" does not apply.


----------- Start Original Message -----------
: MT must be carriedout after any PWHT for detectingany stress cracks.
: Regards,
: Madhesan
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window