where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

1108 views
Technical Discussions
Rohit Bafna
,
TCR Engineering Services, India, Joined Sep 2007, 18

Rohit Bafna

,
TCR Engineering Services,
India,
Joined Sep 2007
18
03:08 Sep-19-2007
ToFD - Collection of Postings

As a NDT services company, we routinely provide AUT using ToFD in India and Saudi Arabia. I wanted to give something back to the outstanding forum on ndt.net and thought that one of the best ways will be to create a compilation of answers on ToFD that are so frequently asked on ndt.net. I plan to update this thread as time permits so that we can all benefit from the collective wisdom of the contributors of this forum. Here are links and brief outlines to important discussions on Time of Flight Diffraction:

Sizing a Defect using ToFD
Contributor Suresh on ndt.net writes:
However, over the last 20 years, TOFD has probably been used more in validations, round robin trials et cetera than any other NDT technique. From this, we have established that TOFD is probably the most accurate sizing technique for embedded defects presently available to the world. A recent test for a major oil company we did on some 30 rootcracks in thin walled material, which were compared to physical measurements after destructive testing showed a mean error on height sizing for TOFD of 0.27 mm with a standard deviation of 0.7 mm. The X-Ray results obviously did not give any height measurement. On the length measurement the accuracy of TOFD was 2.6 mm, with a standard deviation of 4.5 mm. For X-Ray the accuracy of the length measurement was -19 mm (undersized) with a standard deviation of 43.5 mm. By the way, X-Ray only revealed 55% of the cracks, whereas TOFD found 97%.
http://www.ndt.net/wshop/forum/messages-1/10417.html

Demonstration of technique as per 2235-9
Contributor Ed Ginzel writes:
The method of sizing (vertical extent?) for CC2235-9 for examining pressure vessels with a thickness over 13 mm needs to be qualified (demonstrated). It states in i)(3) Flaw Sizing. Flaws shall be sized in accordance with a procedure demonstrated to size similar flaws at similar material depths. Alternatively, a flaw may be sized by a supplemental manual technique so long as it has been qualified by the demonstration above.
http://www.ndt.net/wshop/forum/messages-1/12163.html

Dead Zone Calculation
If I were to bet, this thread is the longest and most frequently asked question with respect to ToFD.
Tom Nelligan of Olympus NDT wrote:
Dead zone -- the interval following the excitation pulse in which potential exchoes are obscured by ringdown -- is a property of BOTH the probe and the instrument. The response of any transducer is highly dependent on how it its pulsed. Changing pulse energy, type (spike, square wave, or tone burst), and damping, as well as receiver gain and filtering, will have a significant effect on the excitation pulse ringdown envelope and hence on dead zone length. As others have suggested, your best approach is to simply measure it under your actual test conditions using appropriate reference blocks.
http://www.ndt.net/wshop/forum/messages-1/11193.html

Ed Ginzel wrote
The "missed data" would be the dead zone. This is not actually a function of the wall thickness but instead, the ring time equivalent depth of the pulse. Frequency, probe spacing and angle used can all be factors. A simple calculator is provided as a download on NDT.net to estimate the Dead Zone heights associated with TOFD setups. Go to http://www.ndt.net/article/v10n06/ginzel/ginzel.htm
For it to be 1/3 wall thickness the specimen you are working with is probably very thin.
http://www.ndt.net/wshop/forum/messages-1/12095.html


Smallest detectable flaw using TOFD
Ed Ginzel once again has a truly informative posting where he mentions:
In clean low carbon steel I have “detected” pores on the order of 0.2mm diameter using a 5MHz TOFD. That is on the order of 5-6 times smaller than the wavelength! But when the same TOFD technique is applied to austenitic stainless steel with grain size on the order of 50-100 microns, the scatter makes it virtually impossible to detect anything but the largest of flaws. Grain size in chrome stainless steels are typical of this order of magnitude. (see http://www.ultrasonic.de/abstract/wcndt96/data2/165.htm)

He further adds:
Properties of the materials tested (not just the alloy, since an alloy may be made in many forms of different grain sizes) and the purpose of the test will be critically important factors when considering the answer to your question. We can discuss “theoretical” limits to “detections”; but in UT (including and especially in TOFD) the response of the indication of concern over the background scatter noise from grain structure will be crucial. If you are expecting to RELIABLY “detect” flaws smaller than the grain size you will probably not be successful. The lateral wave will cause you problems at the lower end of thicknesses due to the dead zone (but I have seen shear wave TOFD used on 4mm wall in fine grained zirconium tubing). Thick sections (200-300mm) can also be tested by TOFD but accumulation of scatter increases with increasing soundpaths. In all cases the signal to noise ratio you can achieve will be the limiting factor for practical use of TOFD.
http://www.ndt.net/wshop/forum/messages-1/11227.html

LoF vs. Slag when doing ToFD as per B31.3 in Piping
J. Mark Davis wrote:
LOF being a planar defect will tend to have a fast rise and fall time, and a short pulse duration. Slag is a volumetric defect and tends to have a slow rise and a long duration. Both defects can cause a beam redirection to the OD or the ID. Also, please realize that as with radiography, you can have several people look at a radiograph and make a slag or a LOF call, and sometimes not all will be in agreement. The same will hold true with UT and Phased Array. If the indication plots to the weld fusion line this probably is side wall lack of fusion. If the indication plots to the weld centerline, line this is probably Slag. Plus, you still analyze Rise and Fall and Pulse Duration.
http://www.ndt.net/wshop/forum/messages-1/11467.html

Code Case 181
A lot people were searching for the actual code case 181 for ToFD. John O'Brien gave the URL to be as http://cstools.asme.org/csconnect/pdf/CommitteeFiles/15243.pdf on the page
http://www.ndt.net/wshop/forum/messages-1/12418.html

ToFD working Style
Rohit Bafna of TCR Engineering Services wrote:
We perform ToFD Services in India and Saudi Arabia and have a two member team. The first team member does the scanning (we are doing ToFD projects as per API 650 appendix u, Code case 181 for piping as well as code case 2235-9) while the second person has a manual UT machine with him. Prior to the start of any project we give out two documents:
- Procedure for examination
- ToFD operating guide for inspectors which illustrates the step by step machine operations. It also includes the timelines of work during the day. For example we prefer to do the scanning in the morning and reporting in the afternoon.
http://www.ndt.net/wshop/forum/messages-1/12366.html

I encourage others to update this thread whenever they find any interesting article on ToFD. I hope over time, we can help other inspectors and fellow technicians learn andimprove the usage of ToFD in the industry.


 
 Reply 
 
K.P.SARVAN
NDT Inspector, AUT / PAUT / TOFD
UTQ / IXAR, India, Joined Sep 2011, 15

K.P.SARVAN

NDT Inspector, AUT / PAUT / TOFD
UTQ / IXAR,
India,
Joined Sep 2011
15
10:21 Apr-16-2012
Re: ToFD - Collection of Postings
In Reply to Rohit Bafna at 03:08 Sep-19-2007 (Opening).

Dear Mr.Rohit..,
Thank you very much for your Interest about others.
You did a Nice job for all of our Colleagues.
Regards,
K.P.Sarvan

 
 Reply 
 

Product Spotlight

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window