ULTRASONIC INSPECTION OF WOODEN UTILITY POLES

I am seeking information on inspecting wooden utility
poles to determine the "life remaining" and "quantity of
decay". Also, where equipment such as the "sylvatest" or
similar low frequency ultrasonic equipment may be
purchased? Thank you.


 
 Reply 
 
Risto Backman
Risto Backman
00:17 Dec-10-1999
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES

I am seeking information on inspecting wooden utility
Also, where equipment such as the "sylvatest" or
similar low frequency ultrasonic equipment may be
purchased? Thank you.

Actually, we are interested in more info. as well as any lab result has been gained from this machine.

Ofcourse we need yr quotation and delivery time.




 
 Reply 
 
Ahmed Mubarrazi
Ahmed Mubarrazi
03:50 May-02-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
: I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.




 
 Reply 
 
Jerry
Jerry
01:20 May-11-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
:Try Engineering Data Management (EDM) in Fort Collins, CO. Good luck.

I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.




 
 Reply 
 
Stephen Bracegirdle
Sales
OIS Engineering Ltd, United Kingdom, Joined Feb 2000, 5

Stephen Bracegirdle

Sales
OIS Engineering Ltd,
United Kingdom,
Joined Feb 2000
5
00:16 May-12-2000
Re: ULTRASONIC INSPECTION OF WOODEN UTILITY POLES
: I am seeking information on inspecting wooden utility
: poles to determine the "life remaining" and "quantity of
: decay". Also, where equipment such as the "sylvatest" or
: similar low frequency ultrasonic equipment may be
: purchased? Thank you.

OIS Engineering has a field portable scanning jig for inspecting utility poles using digital radiography with CT. For further info please email me at seb@oisel.co.uk




 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>