07:15 Dec-17-1999
UT flaw detector

I need information about:

1. calibration of ultrasonic flaw detector EPOCH III-MODEL2300 (PANAMETRIC):

1.A. Initial settings
1.B. Straight beam calibration
1.C. Angle beam transducer calibration.
1.D. Verification of linearity.
1.E. What kind of calibrations block I should use?

And all data about operation of ultrasonic flaw detector epcho III-model 2300 (Panametric). I'll be glad you send me, all information at perezt@texaco.com E-mail.

Thank you very much.

Regards

T.Perez A.




 
 Reply 
 
Ing. Manuel Haces
Ing. Manuel Haces
08:01 Dec-17-1999
Re: UT flaw detector



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
00:04 Dec-18-1999
Re: UT flaw detector
ck the specification that you need to test against, and see what the operator qualification requirements are.

The training and experience requirements were taken directly from the recommended practice for NDT training from the American Society of Nondestructive Testing (ASNT), document SNT-TC-1A.

Godfrey Hands



 
 Reply 
 
Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
02:49 Dec-19-1999
Re: UT flaw detector



 
 Reply 
 
Eng. Fathi Ghanameh
Eng. Fathi Ghanameh
01:30 Dec-22-1999
Re: UT flaw detector



 
 Reply 
 
Bambang Wahyudi
Bambang Wahyudi
05:38 Aug-10-2000
Re: UT flaw detector



 
 Reply 
 
Bambang Wahyudi
Bambang Wahyudi
01:00 Apr-08-2001
Re: UT flaw detector
: : I need information about:

: : 1. calibration of ultrasonic flaw detector EPOCH III-MODEL2300 (PANAMETRIC):

: : 1.A. Initial settings
: : 1.B. Straight beam calibration
: : 1.C. Angle beam transducer calibration.
: : 1.D. Verification of linearity.
: : 1.E. What kind of calibrations block I should use?

: : And all data about operation of ultrasonic flaw detector epcho III-model 2300 (Panametric). I'll be glad you send me, all information at perezt@texaco.com E-mail.

: : Thank you very much.

: : Regards

: : T.Perez A.

: : I am a consultant trainer for Panametrics. I agree with a previous comment that you should contact Panametrics or your Panametrics distributor. You should attend panametrics training. You actually need 80 hours of training in ultrsonics theory, applications, and use. Panametrics can provide the training and the training on the EPOCH III.

: Good Luck,

: J. Mark Davis

I need information about Panametrics DL 36 plus.

Thx
Bambang Wahyudi




 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
01:04 Apr-09-2001
Re: UT flaw detector
: : : I need information about:
.
: : : 1. calibration of ultrasonic flaw detector EPOCH III-MODEL2300 (PANAMETRIC):
.
: : : 1.A. Initial settings
: : : 1.B. Straight beam calibration
: : : 1.C. Angle beam transducer calibration.
: : : 1.D. Verification of linearity.
: : : 1.E. What kind of calibrations block I should use?
.
: : : And all data about operation of ultrasonic flaw detector epcho III-model 2300 (Panametric). I'll be glad you send me, all information at perezt@texaco.com E-mail.
.
: : : Thank you very much.
.
: : : Regards
.
: : : T.Perez A.
.
: : : I am a consultant trainer for Panametrics. I agree with a previous comment that you should contact Panametrics or your Panametrics distributor. You should attend panametrics training. You actually need 80 hours of training in ultrsonics theory, applications, and use. Panametrics can provide the training and the training on the EPOCH III.
.
: : Good Luck,
.
: : J. Mark Davis
.
: I need information about Panametrics DL 36 plus.
.
: Thx
: Bambang Wahyudi

Dear Sirs,

I am the resident Epoch 3 and 36dlplus expert for Panametrics in Australia. I have several hundred calibration settings for the Epoch 3 and can offer the basic settings to you to get you started on your Epoch 3 instrument. I can also offer other training information as your needs arise.

Please send me a personal email to

hermanutzd@panametrics.com.au

with your company details, panametric equipment model numbers (probes and calibration blocks )and I will endeavor to assist you and also put you in contact with your nearest Panametrics expert.

Best Regards.

David Hermanutz
Panametrics Melbourne



 
 Reply 
 
Tran Ngoc Minh
Tran Ngoc Minh
01:12 Apr-09-2001
Re: UT flaw detector
Dear Sir
: : I need information about:

: : 1. calibration of ultrasonic flaw detector EPOCH III-MODEL2300 (PANAMETRIC):

: : 1.A. Initial settings
: : 1.B. Straight beam calibration
: : 1.C. Angle beam transducer calibration.
: : 1.D. Verification of linearity.
: : 1.E. What kind of calibrations block I should use?

: : And all data about operation of ultrasonic flaw detector epcho III-model 2300 (Panametric). I'll be glad you send me, all information at perezt@texaco.com E-mail.

: : Thank you very much.

: : Regards

: : T.Perez A.

: : I am a consultant trainer for Panametrics. I agree with a previous comment that you should contact Panametrics or your Panametrics distributor. You should attend panametrics training. You actually need 80 hours of training in ultrsonics theory, applications, and use. Panametrics can provide the training and the training on the EPOCH III.

: Good Luck,

: J. Mark Davis




 
 Reply 
 
florian rutahindurwa
florian rutahindurwa
02:08 Jan-11-2002
Re: UT flaw detector
kindly please facilitate me with information on the method (and the method itself) of determining nodularity in ductile iron castings using the UT detector


 
 Reply 
 
Santiago Duran
Santiago Duran
00:38 Sep-01-2002
informations
I want to buy a ultrasonic flaw detector used....
diferent option panametric epoch series, krautkramer
give me de the best price...
thanks...


 
 Reply 
 
A. Gkiokas
NDT Inspector, Consultant (Level 3)
NDT TECHNOLOGY, Greece, Joined Aug 2001, 2

A. Gkiokas

NDT Inspector, Consultant (Level 3)
NDT TECHNOLOGY,
Greece,
Joined Aug 2001
2
01:58 Sep-03-2002
Re: informations
: I want to buy a ultrasonic flaw detector used....
: diferent option panametric epoch series, krautkramer
: give me de the best price...
: thanks...
.

Krautkramer USN-52 - 6350 Euro


 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window