Queries on Ultrasonic Testing

Dear Friends,

I have two queries as below and would really appreciate some detailed feedback, which would be helpful to us.

(1) A FBH reflects reflects differently to a logitudinally drilled hole. In Automated Bar Testing (Forge Quality Bar Stock/Bearing Quality Steels etc), we use axially drilled holes to judge the dynamic capability of the ultrasonic testing systems. The fault size in FBH is reached by increasing the testing sensitivity by a calculated factor. How is this factor arrived at? How should we co-relate that a particular size FBH reflection will be equivalent to so & so size of drill hole?

(2) Can anyone share with us the data or standards information about class AA MIL STD-2154 which is 2/64” FBDH. This is used for aircraft double Vac Arc quality. Does this standard call for manual test or automated testing?

Thanks in advance and wishes for a happy holiday season & a great New Year ahead !

Best Regards
Hitesh Mohanlal


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1303

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1303
00:42 Dec-27-2007
Re: Queries on Ultrasonic Testing
I do not have a copy of the MIL standard 2154 so cannot speak to that item.
However, equivalent responses have been reasonably well explained by Prof. I.N. Ermolov. You can go to the article at http://www.ndt.net/article/v07n01/ginzel/ginzel.htm where you will find a utility to compare how a FBH compares to a SDH.


----------- Start Original Message -----------
: Dear Friends,
: I have two queries as below and would really appreciate some detailed feedback, which would be helpful to us.
: (1) A FBH reflects reflects differently to a logitudinally drilled hole. In Automated Bar Testing (Forge Quality Bar Stock/Bearing Quality Steels etc), we use axially drilled holes to judge the dynamic capability of the ultrasonic testing systems. The fault size in FBH is reached by increasing the testing sensitivity by a calculated factor. How is this factor arrived at? How should we co-relate that a particular size FBH reflection will be equivalent to so & so size of drill hole?
: (2) Can anyone share with us the data or standards information about class AA MIL STD-2154 which is 2/64” FBDH. This is used for aircraft double Vac Arc quality. Does this standard call for manual test or automated testing?
: Thanks in advance and wishes for a happy holiday season & a great New Year ahead !
: Best Regards
: Hitesh Mohanlal
------------ End Original Message ------------




 
 Reply 
 
Boiangiu Valentin
Boiangiu Valentin
03:34 Jan-05-2008
Re: Queries on Ultrasonic Testing

Please check the KTA references from http://www.kta-gs.de/e/standards/3200/3201_1e.pdf annex B2.3 b) for the conversion of side drilled hole(Dz) to circular disk reflector (Dksr) used for manual examinations.

The MIL STD-2154 is now cancelled and replaced with ASTM 2375. Please check http://69.7.224.88/viewnews.aspx?newsID=990

Best regards
Valentin

----------- Start Original Message -----------
: Dear Friends,
: I have two queries as below and would really appreciate some detailed feedback, which would be helpful to us.
: (1) A FBH reflects reflects differently to a logitudinally drilled hole. In Automated Bar Testing (Forge Quality Bar Stock/Bearing Quality Steels etc), we use axially drilled holes to judge the dynamic capability of the ultrasonic testing systems. The fault size in FBH is reached by increasing the testing sensitivity by a calculated factor. How is this factor arrived at? How should we co-relate that a particular size FBH reflection will be equivalent to so & so size of drill hole?
: (2) Can anyone share with us the data or standards information about class AA MIL STD-2154 which is 2/64” FBDH. This is used for aircraft double Vac Arc quality. Does this standard call for manual test or automated testing?
: Thanks in advance and wishes for a happy holiday season & a great New Year ahead !
: Best Regards
: Hitesh Mohanlal
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>