WPS

Dear All,

Please help me ? Code/ Standard: ASME IX/ ASME B31.3

If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?

Many thanks for your support.



    
 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
02:15 Dec-28-2007
Re: WPS
Dear Du Xuan Binh

Is your English good enough to read the Codes (it certainly seems quite good from your post) or is there a Vietnamese translation of the Codes? From your profile you work for BP they must have a good technical library.

Access the quoted code and read it - in the long run it will serve you better than being given answers from sources you have no knowledge of. This is an NDT forum, members cannot be expected to have sound knowledge of Code welding rules. AWS has a website with a technical forum or you can try Eng Tips.

---------- Start Original Message -----------
: Dear All,
: Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: Many thanks for your support.
------------ End Original Message ------------




    
 
 Reply 
 
G.Madhesan
Consultant, Welding ýnspector/QAQC inspector
CHENNAI UNIVERSITY, Turkey, Joined Nov 2004, 10

G.Madhesan

Consultant, Welding ýnspector/QAQC inspector
CHENNAI UNIVERSITY,
Turkey,
Joined Nov 2004
10
04:54 Dec-29-2007
Re: WPS
A333 Gr.6 material is different from API 5L X60 material.At any temperature it will not be qualified to each other.


----------- Start Original Message -----------
: Dear Du Xuan Binh
: Is your English good enough to read the Codes (it certainly seems quite good from your post) or is there a Vietnamese translation of the Codes? From your profile you work for BP they must have a good technical library.
: Access the quoted code and read it - in the long run it will serve you better than being given answers from sources you have no knowledge of. This is an NDT forum, members cannot be expected to have sound knowledge of Code welding rules. AWS has a website with a technical forum or you can try Eng Tips.
: ---------- Start Original Message -----------
: : Dear All,
: : Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: : If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: : Many thanks for your support.
------------ End Original Message------------




    
 
 Reply 
 
Welding Guy
Welding Guy
04:01 Dec-30-2007
Re: WPS
----------- Start Original Message -----------
: Dear All,
: Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: Many thanks for your support.
------------ End Original Message ------------

I believe this has already been posted on the AWS forum and answered.
I believe this was the answer you got:

A333, Gr 6 is P1, Gr. 1, and API 5L X60 is P1, Gr. 2.

Since you mention CVN's the answer is "no" A333, Gr. 6 does not qualify API 5L, X60, see QW-403.5; supplementary essential variable.


    
 
 Reply 
 
victorsteel
victorsteel
19:37 Aug-25-2014
Re: WPS
In Reply to Welding Guy at 04:01 Dec-30-2007 .

u will get all Standard and grades of api 5lx60 on http://www.api5lx60.com/

    
 
 Reply 
 

Product Spotlight

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window