Dear All,

Please help me ? Code/ Standard: ASME IX/ ASME B31.3

If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?

Many thanks for your support.



 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
02:15 Dec-28-2007
Re: WPS
Dear Du Xuan Binh

Is your English good enough to read the Codes (it certainly seems quite good from your post) or is there a Vietnamese translation of the Codes? From your profile you work for BP they must have a good technical library.

Access the quoted code and read it - in the long run it will serve you better than being given answers from sources you have no knowledge of. This is an NDT forum, members cannot be expected to have sound knowledge of Code welding rules. AWS has a website with a technical forum or you can try Eng Tips.

---------- Start Original Message -----------
: Dear All,
: Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: Many thanks for your support.
------------ End Original Message ------------




 
 Reply 
 
G.Madhesan
Consultant, Welding ýnspector/QAQC inspector
CHENNAI UNIVERSITY, Turkey, Joined Nov 2004, 10

G.Madhesan

Consultant, Welding ýnspector/QAQC inspector
CHENNAI UNIVERSITY,
Turkey,
Joined Nov 2004
10
04:54 Dec-29-2007
Re: WPS
A333 Gr.6 material is different from API 5L X60 material.At any temperature it will not be qualified to each other.


----------- Start Original Message -----------
: Dear Du Xuan Binh
: Is your English good enough to read the Codes (it certainly seems quite good from your post) or is there a Vietnamese translation of the Codes? From your profile you work for BP they must have a good technical library.
: Access the quoted code and read it - in the long run it will serve you better than being given answers from sources you have no knowledge of. This is an NDT forum, members cannot be expected to have sound knowledge of Code welding rules. AWS has a website with a technical forum or you can try Eng Tips.
: ---------- Start Original Message -----------
: : Dear All,
: : Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: : If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: : Many thanks for your support.
------------ End Original Message------------




 
 Reply 
 
Welding Guy
Welding Guy
04:01 Dec-30-2007
Re: WPS
----------- Start Original Message -----------
: Dear All,
: Please help me ? Code/ Standard: ASME IX/ ASME B31.3
: If I qualify a WPS for A333 Gr6 at charpy -46 0c that can also qualify API X 60 ?
: Many thanks for your support.
------------ End Original Message ------------

I believe this has already been posted on the AWS forum and answered.
I believe this was the answer you got:

A333, Gr 6 is P1, Gr. 1, and API 5L X60 is P1, Gr. 2.

Since you mention CVN's the answer is "no" A333, Gr. 6 does not qualify API 5L, X60, see QW-403.5; supplementary essential variable.


 
 Reply 
 
victorsteel
victorsteel
19:37 Aug-25-2014
Re: WPS
In Reply to Welding Guy at 04:01 Dec-30-2007 .

u will get all Standard and grades of api 5lx60 on http://www.api5lx60.com/

 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window