05:08 Jan-02-2008
About pulsed eddy current testing

What is principle of pulsed eddy current?
What are the differences to the traditional method?


 
 Reply 
 
Catalin Mandache
Catalin Mandache
05:12 Jan-03-2008
Re: About pulsed eddy current testing
Hi Alan,

Here are the main differences (there are many others):
- Pulsed (or Transient) eddy current uses a square wave or step function excitation instead of a sinusoidal one, as used for conventional eddy current testing.
- The received pulsed eddy current signal response is usually represented in the time domain (as with ultrasonic waves testing); conventional eddy current instruments use the impedance plane diagram for signal representation.

The biggest advantage of pulsed eddy current testing comes from deeper penetrability than in conventional technique. This is due mainly to the rich frequency content in a square wave, but also to the large diameter types of excitation coils used.

Some of these differences are discussed in an article right on this site:
http://www.ndt.net/article/v10n06/mandache/mandache.htm

----------- Start Original Message -----------
: What is principle of pulsed eddy current?
: What are the differences to the traditional method?
------------ End Original Message ------------




 
 Reply 
 
Michael Moles †2014 *1948
, Joined ,
03:48 Jan-03-2008
Re: About pulsed eddy current testing
----------- Start Original Message -----------
: Hi Alan,
: Here are the main differences (there are many others):
: - Pulsed (or Transient) eddy current uses a square wave or step function excitation instead of a sinusoidal one, as used for conventional eddy current testing.
: - The received pulsed eddy current signal response is usually represented in the time domain (as with ultrasonic waves testing); conventional eddy current instruments use the impedance plane diagram for signal representation.
: The biggest advantage of pulsed eddy current testing comes from deeper penetrability than in conventional technique. This is due mainly to the rich frequency content in a square wave, but also to the large diameter types of excitation coils used.
: Some of these differences are discussed in an article right on this site:
: http://www.ndt.net/article/v10n06/mandache/mandache.htm
: : What is principle of pulsed eddy current?
: : What are the differences to the traditional method?
------------ End Original Message ------------

Alan:

Try the following web site: http://www.ndt-ed.org/EducationResources/CommunityCollege/EddyCurrents/AdvancedTechniques/background.htm. This gives a good outline of pulsed eddy currents.

Michael



 
 Reply 
 
Alan
Alan
02:43 Jan-08-2008
Re: About pulsed eddy current testing
Hello Michael,

Thank you!
The web is so useful.
I am new in NDT. It is so good to find friends here.
=]

----------- Start Original Message -----------
: Hi Alan,
: Here are the main differences (there are many others):
: - Pulsed (or Transient) eddy current uses a square wave or step function excitation instead of a sinusoidal one, as used for conventional eddy current testing.
: - The received pulsed eddy current signal response is usually represented in the time domain (as with ultrasonic waves testing); conventional eddy current instruments use the impedance plane diagram for signal representation.
: The biggest advantage of pulsed eddy current testing comes from deeper penetrability than in conventional technique. This is due mainly to the rich frequency content in a square wave, but also to the large diameter types of excitation coils used.
: Some of these differences are discussed in an article right on this site:
: http://www.ndt.net/article/v10n06/mandache/mandache.htm
: : What is principle of pulsed eddy current?
: : What are the differences to the traditional method?
------------ End Original Message ------------




 
 Reply 
 
Alan
Alan
02:47 Jan-08-2008
Re: About pulsed eddy current testing
Hi Catalin,

Thank you for your information.
You must be a expert in ET.

----------- Start Original Message -----------
: Hi Alan,
: Here are the main differences (there are many others):
: - Pulsed (or Transient) eddy current uses a square wave or step function excitation instead of a sinusoidal one, as used for conventional eddy current testing.
: - The received pulsed eddy current signal response is usually represented in the time domain (as with ultrasonic waves testing); conventional eddy current instruments use the impedance plane diagram for signal representation.
: The biggest advantage of pulsed eddy current testing comes from deeper penetrability than in conventional technique. This is due mainly to the rich frequency content in a square wave, but also to the large diameter types of excitation coils used.
: Some of these differences are discussed in an article right on this site:
: http://www.ndt.net/article/v10n06/mandache/mandache.htm
: : What is principle of pulsed eddy current?
: : What are the differences to the traditional method?
------------ End Original Message ------------




 
 Reply 
 
Riccardo Scottini
Riccardo Scottini
04:39 Jan-11-2008
Re: About pulsed eddy current testing
Hi Alan,

Our Pulsed Eddy Current equipment is called RTD-INCOTEST, where INCOTEST is an acronym for INsulated COmponent TESTing. The principle of pulsed Eddy Current is that once a stable magnetic field is created with a sending coil (DC current) in the carbon steel plate under examination. The sending circuit is opened and the receiving coil record the signal of the Eddy Currents induced in the base material during this "transitorium". No Eddy Current is induced when the magnetic field is constant. These are induced when the Magnetic Field changes therefore during the “transitorium”.
The technique does not need any contact or special cleaning and may is efficient through insulation and weather proofing even of Galvanised cladding or through fire proofing and coating. The equipment needs the object under examination to be ferromagnetic, therefore Carbon Steel or Low Alloy Carbon Steel.
The main difference with traditional Eddy Current Methods is that mostly they measures continuously and they are mainly performed on not Ferro materials and INCOTEST needs a ferro base material and it is perform with steady measurement because on each measurement position the induced DC magnetic field must first get uniform and constant, once this condition is reached (some ms) the equipment “listen” to the transitorium (some ms) and only after that the probe may be replaced to the next position. Other difference is that INCOTEST gives Average Wall Thickness values in a lift-off range up to 200mm and may inspect WT up to 65mm.

I linked our INCOTEST site where you may find more information also regarding the technology main applications.

Any question… feel free to contact me.
Regards
Riccardo




 
 Reply 
 
karthikeyan.J
karthikeyan.J
05:29 Jan-26-2008
Re: About pulsed eddy current testing

What is principle of pulsed eddy current?
What are the differences to the traditional method?
what is the difference of the eddy current from other NDT methods?


 
 Reply 
 

Product Spotlight

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window