Fireside Tubesheet Inspection

We have waste heat boilers with 12m long horizontal tubes 78mm dia x 6mm wt expanded and seal welded between tube sheets - hot side / cold side. The hot side tube sheet is refractory clad with a ceramic insert in the tubes.
Our RBI requires that we conduct inspection.
What would be the best NDT method to locate cracking at tube to tubesheet junction, and corrosion / erosion of the tubes.
There is access only from the tube I.D. and tubesheet face on the cold side.


 
 Reply 
 
ranjeet singh
Engineering, Asst.Manager-Condition Monitoring
TATA chemicals ltd.(fertilizer div.), India, Joined May 2006, 6

ranjeet singh

Engineering, Asst.Manager-Condition Monitoring
TATA chemicals ltd.(fertilizer div.),
India,
Joined May 2006
6
04:57 Feb-12-2008
Re: Fireside Tubesheet Inspection
Mr.Collin Maloney ,
for tube corossion and erosion ,you may select tube inspection technique like RFET or IRIS
For knowing health of ferrule or tube ID surface you may go for Fiberscopy/boroscope
for ascertaining health of TTS joint ,go for Helium leak testing if possible else do DPT or visual inspection.

Regards

----------- Start Original Message -----------
: We have waste heat boilers with 12m long horizontal tubes 78mm dia x 6mm wt expanded and seal welded between tube sheets - hot side / cold side. The hot side tube sheet is refractory clad with a ceramic insert in the tubes.
: Our RBI requires that we conduct inspection.
: What would be the best NDT method to locate cracking at tube to tubesheet junction, and corrosion / erosion of the tubes.
: There is access only from the tube I.D. and tubesheet face on the cold side.
------------ End Original Message ------------




 
 Reply 
 
Kåre Johansson
Kåre Johansson
09:49 Feb-12-2008
Re: Fireside Tubesheet Inspection
----------- Start Original Message -----------
We have a simillar challenge on our plant and have found a cobination of methodes to be the most effective.

As mentioned by the previous reply some ET techniques will work well, discuss the details with a good inspection company and provide as many details as possible. IRIS will work, but I am sceptical unless you can guarantee against damage to the refractory and ferrules.

We have good experience using video techniques, including laser meassurements of roundness/deformation of the tubes.

Leak testing of the seal welds is a good idea, but then you must have some access to the shell side of the bundle and this wil probably not tell you much about the welds on the hot face. If you have access on the shell side og the tubes I would reccommend you try to do a video inspection on the tubes as close to the hot face as possible. There must be some drain in the shell?

PT/MT and visual inspection of accessible welds is natural if you have seal weld. As you are inside a vesel I would prefere flurorecent techniques. Again you have the problem of lack of access to the hot face.

In my experience all troubles with this type of boilers originate on the waterside. Your best bet is to enforce a VERY STRICT water chemistry.
regards
Kåre Johansson

: Mr.Collin Maloney ,
: for tube corossion and erosion ,you may select tube inspection technique like RFET or IRIS
: For knowing health of ferrule or tube ID surface you may go for Fiberscopy/boroscope
: for ascertaining health of TTS joint ,go for Helium leak testing if possible else do DPT or visual inspection.
: Regards
: : We have waste heat boilers with 12m long horizontal tubes 78mm dia x 6mm wt expanded and seal welded between tube sheets - hot side / cold side. The hot side tube sheet is refractory clad with a ceramic insert in the tubes.
: : Our RBI requires that we conduct inspection.
: : What would be the best NDT method to locate cracking at tube to tubesheet junction, and corrosion / erosion of the tubes.
: : There is access only from the tube I.D. and tubesheet face on the cold side.
------------ End Original Message ------------




 
 Reply 
 
Tony McMurtry
Tony McMurtry
20:10 Mar-01-2009
Re: Fireside Tubesheet Inspection
In Reply to Kåre Johansson at 09:49 Feb-12-2008 .

While water management can be a problem using IRIS around refactory, a little prior planning can keep the problem under control. Internal/external erosion/corrosion can best be identified and quantified with the IRIS unit. IRIS cannot determine if cracking is
present. The inserts would prevent the tube areas beneath from being properly inspected.

 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window