Information redarding Material

During the NDT inspection of a pump shaft key I rejected the key due to cracking. The material of the key was A276 - 316. Now to machine a new key material 316 is not available
My question is that can we use SS 316L, 304, or 304L instead of SS316 or what is the better alternate.

Thanks & Regards
Muhammad Azhar Jamil Khan



 
 Reply 
 
Collin Maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

Collin Maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
06:19 Feb-23-2008
Re: Information redarding Material
----------- Start Original Message -----------
: During the NDT inspection of a pump shaft key I rejected the key due to cracking. The material of the key was A276 - 316. Now to machine a new key material 316 is not available
: My question is that can we use SS 316L, 304, or 304L instead of SS316 or what is the better alternate.
:
: Thanks & Regards
: Muhammad Azhar Jamil Khan
------------ End Original Message ------------

Azhar
The info you have quoted is for 316 S/Steel bar stock. I would suggest that you need to find out the shear strength for A276-316 and find a comparable material on that basis. I think that you will find that 316 plate is Ok!


 
 Reply 
 

Product Spotlight

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window