Ahtram
Sales
Sanco, United Arab Emirates (UAE), Joined Jan 2008, 4

Ahtram

Sales
Sanco,
United Arab Emirates (UAE),
Joined Jan 2008
4
09:38 Feb-10-2008
Which one is the best NDT/PMI metal analyser?

I am assuming most of you guys have used NDT metal analysers from Niton, Oxford Instruments and Innovex.

So would anyone like to share there experience with the metal analysers mentioned above?

Which one you think is the best and why?




 
 Reply 
 
burhanudin sudharmin
Engineering, Reliability and Integrity Eng
Shell Malaysia Trading, Malaysia, Joined Jan 2008, 54

burhanudin sudharmin

Engineering, Reliability and Integrity Eng
Shell Malaysia Trading,
Malaysia,
Joined Jan 2008
54
05:17 Feb-11-2008
Re: Which one is the best NDT/PMI metal analyser?
Which one is the best, is quite subjective to one's need and requirements.
Just to share, I have experience in the use of the Texas Instruments Alloy Analyser. Its however, limited to identifying alloys only. The other downside is the use of radioactive isotopes which requires replacement in about 5 years due to its half life, and maintenance upkeep could be expensive.

----------- Start Original Message -----------
: I am assuming most of you guys have used NDT metal analysers from Niton, Oxford Instruments and Innovex.
: So would anyone like to share there experience with the metal analysers mentioned above?
: Which one you think is the best and why?
------------ End Original Message ------------




 
 Reply 
 
ahtram
Sales
Sanco, United Arab Emirates (UAE), Joined Jan 2008, 4

ahtram

Sales
Sanco,
United Arab Emirates (UAE),
Joined Jan 2008
4
01:22 Feb-13-2008
Re: Which one is the best NDT/PMI metal analyser?
----------- Start Original Message -----------
: Which one is the best, is quite subjective to one's need and requirements.
: Just to share, I have experience in the use of the Texas Instruments Alloy Analyser. Its however, limited to identifying alloys only. The other downside is the use of radioactive isotopes which requires replacement in about 5 years due to its half life, and maintenance upkeep could be expensive.
: : I am assuming most of you guys have used NDT metal analysers from Niton, Oxford Instruments and Innovex.
: : So would anyone like to share there experience with the metal analysers mentioned above?
: : Which one you think is the best and why?
------------ End Original Message ------------

hmmm thanks burhanudin. Yes I agree with you there is a downside to the use of radioactive isptopes where it requies a replacement. Also I do believe radioactive isotopes happen to be dangerous to humans if humans are exposed to them. Radioactive source is old technology banned in USA and europe. its a shame that companies like Niton sell radioactive source metal analysers in the Middle East where there are no legislations against radioactive source. Maybe in the future there will be.




 
 Reply 
 
mj
mj
04:29 Feb-17-2008
Re: Which one is the best NDT/PMI metal analyser?
----------- Start Original Message -----------
: : Which one is the best, is quite subjective to one's need and requirements.
: : Just to share, I have experience in the use of the Texas Instruments Alloy Analyser. Its however, limited to identifying alloys only. The other downside is the use of radioactive isotopes which requires replacement in about 5 years due to its half life, and maintenance upkeep could be expensive.
: : : I am assuming most of you guys have used NDT metal analysers from Niton, Oxford Instruments and Innovex.
: : : So would anyone like to share there experience with the metal analysers mentioned above?
: : : Which one you think is the best and why?
: hmmm thanks burhanudin. Yes I agree with you there is a downside to the use of radioactive isptopes where it requies a replacement. Also I do believe radioactive isotopes happen to be dangerous to humans if humans are exposed to them. Radioactive source is old technology banned in USA and europe. its a shame that companies like Niton sell radioactive source metal analysers in the Middle East where there are no legislations against radioactive source. Maybe in the future there will be.
------------ End Original Message ------------

if some one don't know about the radiation problems better plz don't talk.... if compare with industrial radiograpy, its very very low... so its not the matter of radiation, its the matter of refilling and limitation of indentification, mean time oxford provide some good equipment with argon to find even carbon and ph., looks nice but the problem there also.... i have 2 oxford equipment. which will brakedown every 6 months or 7 months... to get equipment after repair manufacture usualy take 3-4 months... but quipmentwise ARCMet 930 ( old Mechine0 is good
Thanks


 
 Reply 
 
jason
jason
04:51 Mar-14-2008
Re: Which one is the best NDT/PMI metal analyser?
----------- Start Original Message -----------
: : : Which one is the best, is quite subjective to one's need and requirements.
: : : Just to share, I have experience in the use of the Texas Instruments Alloy Analyser. Its however, limited to identifying alloys only. The other downside is the use of radioactive isotopes which requires replacement in about 5 years due to its half life, and maintenance upkeep could be expensive.
: : : : I am assuming most of you guys have used NDT metal analysers from Niton, Oxford Instruments and Innovex.
: : : : So would anyone like to share there experience with the metal analysers mentioned above?
: : : : Which one you think is the best and why?
: : hmmm thanks burhanudin. Yes I agree with you there is a downside to the use of radioactive isptopes where it requies a replacement. Also I do believe radioactive isotopes happen to be dangerous to humans if humans are exposed to them. Radioactive source is old technology banned in USA and europe. its a shame that companies like Niton sell radioactive source metal analysers in the Middle East where there are no legislations against radioactive source. Maybe in the future there will be.
: if some one don't know about the radiation problems better plz don't talk.... if compare with industrial radiograpy, its very very low... so its not the matter of radiation, its the matter of refilling and limitation of indentification, mean time oxford provide some good equipment with argon to find even carbon and ph., looks nice but the problem there also.... i have 2 oxford equipment. which will brakedown every 6 months or 7 months... to get equipment after repair manufacture usualy take 3-4 months... but quipmentwise ARCMet 930 ( old Mechine0 is good
: Thanks
------------ End Original Message ------------

I used the dual source Nitons for NACE MR0175 certification and weld/parent mat"l alloy composition and was very impressed. Compared to the competition they are small, lightweight and fast. I used them in Alberta, Canada and they performed well in extreme conditions. I would recommend them for field work. I'm not sure if they would be the right tool for a lab environment since I try to stay
out of the lab rat zone.

Cheers



 
 Reply 
 
Aage
Aage
16:04 Mar-11-2009
Re: Which one is the best NDT/PMI metal analyser?
In Reply to jason at 04:51 Mar-14-2008 .

Just a follow up on isotope vs. X-ray tube. Isotopes currently being used have much longer lifetime than those used some years ago. They are now described as "everlasting" having half-life of about 100 years. The Niton XLp818 would be an example of such model.
X-ray tube is more accurate and faster than isotope.
X-ray tube models may be easier to transport (e.g. on planes) than isotope models. The rules for this vary from country to country, also within Europe. I believe some countries do not allow the use of isotopes (e.g. Spain). However, I live in Norway and consider buying an isotope based model due to lifetime and that I will only use it on high alloyed steels, and thus I do not need the increased accuracy of the X-ray tube.

 
 Reply 
 

Product Spotlight

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

On Demand Webinar: Using Eddy Current Array for Large Areas in Place of Magnetic Particle and Liquid Penetrant Testing

New on-demand webinar on the use of eddy current array (ECA) technology in lieu of liquid penetrant
...
testing (PT) and magnetic particle testing (MT) for large area screenings. The webinar includes an introduction to the technologies with advantages and disadvantages of each. Side by side examples are discussed including aircraft stringers, engine blades, forgings, weld plates & more. View it today.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window